IMR OpenIR
Effect of substituting Mn for Ni on the hydrogen storage and electrochemical properties of ReNi2.6-xMnxCo0.9 alloys
Jiang, Long1,2; Li, Guangxu1; Xu, Liqin1; Jiang, Weiqing1; Lan, Zhiqiang1; Guo, Jin1,3
通讯作者Guo, Jin(guojin@gxu.edu.cn)
2010
发表期刊INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
ISSN0360-3199
卷号35期号:1页码:204-209
摘要ReNi2.6-xMnxCo0.9 (x = 0.0, 0.225, 0.45, 0.675, 0.90) alloys were prepared by induction melting. The effects of partially substituting Mn for Ni on the phase structure and electrochemical properties of the alloys were investigated systematically. In the alloys, (La, Ce)(2)Ni-7 phase with a Ce2Ni7-type structure, (Pr, Ce)Co-3 phase with a PuNi3-type structure, and (La, Pr)Ni-5 phase with a CaCu5-type structure were the main phases. The (La,Pr)Ni phase appeared when x increased to 0.45, and the (La, Pr)Ni-5 phase disappeared with further increasing x (x > 0.45). The hydrogen-storage capacity of the ReNi2.6-xMnxCo0.9 (x = 0.0, 0.225, 0.45, 0.675, 0.90) alloys initially increased and reached a maximum when Mn content was x = OAS, and then decreased with further increasing Mn content. The ReNi2.6-xMnxCo0.9 (x = 0.0, 0.225, 0.45, 0.675, 0.90) alloy exhibited a hydrogen- storage capacity of 0.81, 0.98, 1.04, 0.83 and 0.53 wt.%, respectively. Electrochemical studies showed that the maximum discharge capacity of the alloy electrodes initially increased from 205 mAh/g (x 0.0) to 352 mAh/g (x = 0.45) and then decreased to 307 mAh/g (x = 90). The hydrogen absorption rate first increased and then decreased with addition of Mn element. The ReNi2.15Mn0.45Co0.9 alloy showed faster hydrogen absorption kinetics than that of the other alloys. The presence of Mn element slowed hydrogen desorption kinetics. (C) 2009 Professor T. Nejat Veziroglu. Published by Elsevier Ltd. All rights reserved.
关键词Hydrogen storage alloy Hydrogen storage property Electrochemical characteristic
资助者National Natural Science Foundation of China ; Natural Science Foundation of Guangxi ; Guangxi University Key Program for Science and Technology Research
DOI10.1016/j.ijhydene.2009.10.041
收录类别SCI
语种英语
资助项目National Natural Science Foundation of China[50561002] ; National Natural Science Foundation of China[50861003] ; Natural Science Foundation of Guangxi[0728028] ; Guangxi University Key Program for Science and Technology Research[2004ZD04]
WOS研究方向Chemistry ; Electrochemistry ; Energy & Fuels
WOS类目Chemistry, Physical ; Electrochemistry ; Energy & Fuels
WOS记录号WOS:000274079200024
出版者PERGAMON-ELSEVIER SCIENCE LTD
引用统计
被引频次:24[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/101936
专题中国科学院金属研究所
通讯作者Guo, Jin
作者单位1.Guangxi Univ, Coll Phys Sci & Technol, Nanning 530004, Peoples R China
2.Yangtze Univ, Sch Phys Sci & Technol, Jinzhou 434023, Peoples R China
3.Chinese Acad Sci, Int Ctr Mat Phys, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Jiang, Long,Li, Guangxu,Xu, Liqin,et al. Effect of substituting Mn for Ni on the hydrogen storage and electrochemical properties of ReNi2.6-xMnxCo0.9 alloys[J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY,2010,35(1):204-209.
APA Jiang, Long,Li, Guangxu,Xu, Liqin,Jiang, Weiqing,Lan, Zhiqiang,&Guo, Jin.(2010).Effect of substituting Mn for Ni on the hydrogen storage and electrochemical properties of ReNi2.6-xMnxCo0.9 alloys.INTERNATIONAL JOURNAL OF HYDROGEN ENERGY,35(1),204-209.
MLA Jiang, Long,et al."Effect of substituting Mn for Ni on the hydrogen storage and electrochemical properties of ReNi2.6-xMnxCo0.9 alloys".INTERNATIONAL JOURNAL OF HYDROGEN ENERGY 35.1(2010):204-209.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Jiang, Long]的文章
[Li, Guangxu]的文章
[Xu, Liqin]的文章
百度学术
百度学术中相似的文章
[Jiang, Long]的文章
[Li, Guangxu]的文章
[Xu, Liqin]的文章
必应学术
必应学术中相似的文章
[Jiang, Long]的文章
[Li, Guangxu]的文章
[Xu, Liqin]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。