Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon
Gan, Y
通讯作者Gan, Y()
2001-06-18
发表期刊ACTA METALLURGICA SINICA
ISSN0412-1961
卷号37期号:6页码:585-588
摘要Dynamic fracture characteristics have been observed and interpreted for Fe-Mo-Si-B amorphous alloy ribbon. Crack branching and stress wave induced cracking are the main features of dynamic fracture. Branching of main crack occurs when the crack tip intensity factor reaches the critical value K-IB = 35 MPa(.)m(1/2), and the corresponding plane strain fracture toughness K-Ic = 16 MPa(.)m(1/2). It is deduced that crack branching is the necessary condition for generation of compressive longitudinal wave. Stress wave induced cracking occurs when the amplitude of reflected compressive longitudinal wave reaches the tensile strength.
关键词amorphous alloy dynamic fracture crack branching stress wave induced cracking (SWIC)
收录类别SCI
语种英语
WOS研究方向Metallurgy & Metallurgical Engineering
WOS类目Metallurgy & Metallurgical Engineering
WOS记录号WOS:000172766900006
出版者SCIENCE CHINA PRESS
引用统计
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/112294
专题中国科学院金属研究所
通讯作者Gan, Y
作者单位Chinese Acad Sci, Met Res Inst, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Gan, Y. Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon[J]. ACTA METALLURGICA SINICA,2001,37(6):585-588.
APA Gan, Y.(2001).Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon.ACTA METALLURGICA SINICA,37(6),585-588.
MLA Gan, Y."Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon".ACTA METALLURGICA SINICA 37.6(2001):585-588.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Gan, Y]的文章
百度学术
百度学术中相似的文章
[Gan, Y]的文章
必应学术
必应学术中相似的文章
[Gan, Y]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。