| High temperature oxidation behavior of (Ni, Pd)Ai coating |
| Li, MJ; Sun, XF; Guan, HG; Jiang, XX; Hu, ZQ
|
通讯作者 | Li, MJ()
|
| 2003-04-11
|
发表期刊 | ACTA METALLURGICA SINICA
 |
ISSN | 0412-1961
|
卷号 | 39期号:4页码:439-443 |
摘要 | The 1100 degreesC oxidation behavior of (Ni,Pd)Al coating prepared by low pressure pack cementation on the nickel-based superalloy M38, was studied by thermal gravimetric analysis (TGA), X-ray diffraction (XRD), SEM. The results show that the oxidation kinetics of (Ni, Pd)Al coating obeys parabolic law and its performance of high temperature oxidation resistance is better than that of plain aluminide coating. The degradation mechanism is similar to NiAl. The addition of Pd is in favor of stabilizing the beta phase, retarding the degradation of coating, and increasing the high temperature oxidation resistance of coating. |
关键词 | (Ni,Pd)Al coating
nickel-based superalloy
high temperature oxidation property
degradation
|
收录类别 | SCI
|
语种 | 英语
|
WOS研究方向 | Metallurgy & Metallurgical Engineering
|
WOS类目 | Metallurgy & Metallurgical Engineering
|
WOS记录号 | WOS:000182921300021
|
出版者 | SCIENCE CHINA PRESS
|
引用统计 |
|
文献类型 | 期刊论文
|
条目标识符 | http://ir.imr.ac.cn/handle/321006/116302
|
专题 | 中国科学院金属研究所
|
通讯作者 | Li, MJ |
作者单位 | Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Peoples R China
|
推荐引用方式 GB/T 7714 |
Li, MJ,Sun, XF,Guan, HG,et al. High temperature oxidation behavior of (Ni, Pd)Ai coating[J]. ACTA METALLURGICA SINICA,2003,39(4):439-443.
|
APA |
Li, MJ,Sun, XF,Guan, HG,Jiang, XX,&Hu, ZQ.(2003).High temperature oxidation behavior of (Ni, Pd)Ai coating.ACTA METALLURGICA SINICA,39(4),439-443.
|
MLA |
Li, MJ,et al."High temperature oxidation behavior of (Ni, Pd)Ai coating".ACTA METALLURGICA SINICA 39.4(2003):439-443.
|
修改评论