AbstractEngineering alloys of heat resistance often generate pores at the scale/alloy interface during high temperature oxidation. The accumulation and growth of those pores greatly weaken scale adhesion. The purpose of this study is to observe pore development in Fe-40%Al (atomic fraction) and measure the change in pore volume with oxidation time. Experimental results are then compared to a theoretical calculation where all vacancies are allowed to condense as voids. After removing the oxide scales formed after various times of oxidation at 1000 degreesC in oxygen, the alloy surface was analyzed using scanning electron microscopy (SEM) and atomic force microscopy (AFM) to determine the size and depth of interfacial pores. Results are discussed in light of possible mechanisms involved in pore formation at scale/alloy interfaces.
Keywordpore interface oxidation FeAl A1(2)O(3)
Indexed BySCI
Language英语
WOS Research AreaMetallurgy & Metallurgical Engineering
WOS SubjectMetallurgy & Metallurgical Engineering
WOS IDWOS:000186451300011
PublisherSCIENCE PRESS
Citation statistics
Cited Times:2[WOS]   [WOS Record]     [Related Records in WOS]
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/117805
Collection中国科学院金属研究所
Corresponding AuthorHou, Y
Affiliation1.Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Peoples R China
2.Lawrence Berkeley Lab, Div Sci Mat, Berkeley, CA 94720 USA
Recommended Citation
GB/T 7714
Niu, Y,Hou, Y. Characterization of pore development at Al(2)O(3/)FeAl interface during high temperature oxidation[J]. ACTA METALLURGICA SINICA,2003,39(10):1065-1070.
APA Niu, Y,&Hou, Y.(2003).Characterization of pore development at Al(2)O(3/)FeAl interface during high temperature oxidation.ACTA METALLURGICA SINICA,39(10),1065-1070.
MLA Niu, Y,et al."Characterization of pore development at Al(2)O(3/)FeAl interface during high temperature oxidation".ACTA METALLURGICA SINICA 39.10(2003):1065-1070.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[Niu, Y]'s Articles
[Hou, Y]'s Articles
Baidu academic
Similar articles in Baidu academic
[Niu, Y]'s Articles
[Hou, Y]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[Niu, Y]'s Articles
[Hou, Y]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.