CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER | |
Wang Jianqiu; Huang Fa; Ke Wei | |
通讯作者 | Ke Wei(kewei@imr.ac.cn) |
2016-10-01 | |
发表期刊 | ACTA METALLURGICA SINICA
![]() |
ISSN | 0412-1961 |
卷号 | 52期号:10页码:1333-1344 |
摘要 | Inconel 690TT and Incoloy 800MA have been widely used as steam generator heat transfer tubes in nuclear power plants (NPPs). The corrosion behaviors of these two alloys in high temperature high pressure water have to be fully addressed. This work systematically studied the microstructures of the as-received Inconel 690TT and Incoloy 800MA steam generator tubes (SGTs) and compared the oxide films formed on the tubing materials in high temperature water using several analytical methods including SEM, EBSD, GIXRD, SAED and STEM. The results show that from outer surface to inner surface of Inconel 690TT SGTs, the deviation degrees from the ideal Sigma 3 misorientation and the average value of Kernel average misorientation (KAM) gradually increase. The outer surface of Inconel 690TT SGTs are weakest. For Incoloy 800MA SGTs, the deviation degrees from the ideal Sigma 3 misorientation are within 0 similar to 1 degrees, and the change of KAM average value is small. Exposed to 325 degrees C pure water containing 0.75x10(-6) O-2 for 720 h, oxide films of both Inconel 690TT SGTs and Incoloy 800MA SGTs have duplex structure. On Inconel 690TT SGTs, the outer layer is Fe-rich spinel and small NiO particles; the inner layer mainly is NiO, porous and less protective with the thickness of 716 nm. On Incoloy 800MA SGTs, the outer layer is big polyhedral spinel; the inner layer is small polyhedral spinel and protective with the average thickness of 150 nm; Cr is enriched at the interface between inner oxide layer and matrix. In high temperature water with dissolved oxygen, due to the preferential dissolution of Cr, Incoloy 800MA is more corrosion resistant than In-conel 690TT. |
关键词 | Inconel 690TT Incoloy 800MA high temperature high pressure water oxide film |
资助者 | National Funds for Distinguished Young Scholars |
DOI | 10.11900/0412.1961.2016.00276 |
收录类别 | SCI |
语种 | 英语 |
资助项目 | National Funds for Distinguished Young Scholars[51025104] |
WOS研究方向 | Metallurgy & Metallurgical Engineering |
WOS类目 | Metallurgy & Metallurgical Engineering |
WOS记录号 | WOS:000390080900017 |
出版者 | SCIENCE PRESS |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/123270 |
专题 | 中国科学院金属研究所 |
通讯作者 | Ke Wei |
作者单位 | Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China |
推荐引用方式 GB/T 7714 | Wang Jianqiu,Huang Fa,Ke Wei. CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER[J]. ACTA METALLURGICA SINICA,2016,52(10):1333-1344. |
APA | Wang Jianqiu,Huang Fa,&Ke Wei.(2016).CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER.ACTA METALLURGICA SINICA,52(10),1333-1344. |
MLA | Wang Jianqiu,et al."CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER".ACTA METALLURGICA SINICA 52.10(2016):1333-1344. |
条目包含的文件 | 条目无相关文件。 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论