IMR OpenIR
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW
Ming Hongliang1,2; Zhang Zhiming1; Wang Jianqiu1; Han En-Hou1; Su Mingxing3
Corresponding AuthorWang Jianqiu(wangjianqiu@imr.ac.cn)
2017
Source PublicationACTA METALLURGICA SINICA
ISSN0412-1961
Volume53Issue:1Pages:57-69
AbstractDissimilar metal weld joints (DMWJ) widely exist in the nuclear power plants to join the different parts which are made of different structural materials. Among these DMWJs, safe-end DMWJ has attracted much attention of researchers and operating enterprises, as premature failures, mainly stress corrosion cracking failures, have occurred in these kinds of joints. However, DMWJ with 52M as filler metal in the nuclear power plants has no in-service experience. To ensure the structural integrity of the weld joint and the safe operation of the future plants, the microstructure and local properties of a domestic safe-end DMWJ by using hot-wire gas tungsten arc welding (GTAW) technology was studied in detail by OM, SEM, micro-hardness testing, local mechanical tensile testing and slow strain rate tests. The tensile tests were performed at room temperature with the tensile speed of 5 mu m/s while the slow strain rate tests were conducted in simulated primary water containing 1500 mg/L B as H3BO3 and 2.3 mg/L Li as LiOH with 2 mg/L dissolved oxygen at 325 degrees C. A large amount of type I boundaries and type II boundaries which are susceptible to stress corrosion cracking (SCC) exist in 52Mb near the SA508/52Mb interface and result in the highest SCC susceptibility of this interface. Microstructure transition was found in the SA508 heat affected zone (HAZ). In 316LN HAZ, increasing the distance from the fusion boundary, the number fraction of CSL boundaries increase while the residual strain decreases, resulting in the second-highest SCC susceptibility of 316LN HAZ. In 52M, residual strain distributes randomly but not uniformly, the residual strain is prone to accumulate at the grain boundaries. Dramatic changes of mechanical properties are observed across the joint, especially at the SA508/52M interface. The differences of the local microstructure and chemical composition lead to the differences of the local properties of the weld joint.
Keyworddissimilar metal weld joint microstructure local mechanical property stress corrosion cracking susceptibility residual strain
Funding OrganizationNational Natural Science Foundation of China ; Science and Technology Commission of Shanghai Municipality ; Key Research Program of Frontier Sciences, CAS
DOI10.11900/0412.1961.2016.00135
Indexed BySCI
Language英语
Funding ProjectNational Natural Science Foundation of China[51301183] ; Science and Technology Commission of Shanghai Municipality[14DZ2250300] ; Key Research Program of Frontier Sciences, CAS[QYZDY-SSW-JSC012]
WOS Research AreaMetallurgy & Metallurgical Engineering
WOS SubjectMetallurgy & Metallurgical Engineering
WOS IDWOS:000393446900007
PublisherSCIENCE PRESS
Citation statistics
Cited Times:22[WOS]   [WOS Record]     [Related Records in WOS]
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/123804
Collection中国科学院金属研究所
Corresponding AuthorWang Jianqiu
Affiliation1.Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Liaoning Key Lab Safety & Assessment Tech Nucl Ma, Shenyang 110016, Peoples R China
2.Univ Chinese Acad Sci, Beijing 100049, Peoples R China
3.Shanghai Res Ctr Weld & Detect Engn Tech Nucl Equ, Shanghai 201306, Peoples R China
Recommended Citation
GB/T 7714
Ming Hongliang,Zhang Zhiming,Wang Jianqiu,et al. Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW[J]. ACTA METALLURGICA SINICA,2017,53(1):57-69.
APA Ming Hongliang,Zhang Zhiming,Wang Jianqiu,Han En-Hou,&Su Mingxing.(2017).Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW.ACTA METALLURGICA SINICA,53(1),57-69.
MLA Ming Hongliang,et al."Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW".ACTA METALLURGICA SINICA 53.1(2017):57-69.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[Ming Hongliang]'s Articles
[Zhang Zhiming]'s Articles
[Wang Jianqiu]'s Articles
Baidu academic
Similar articles in Baidu academic
[Ming Hongliang]'s Articles
[Zhang Zhiming]'s Articles
[Wang Jianqiu]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[Ming Hongliang]'s Articles
[Zhang Zhiming]'s Articles
[Wang Jianqiu]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.