Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 °C Aerated Supercritical Water | |
Alternative Title | Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 °C Aerated Supercritical Water |
Zhong Xiangyu; Wu Xinqiang; Han Enhou | |
2018 | |
Source Publication | Journal of Materials Science & Technology
![]() |
ISSN | 1005-0302 |
Volume | 34Issue:3Pages:561-569 |
Abstract | The oxide films formed on Alloy 690 exposed to 600 °C supercritical water were characterized using mass measurement, X-ray diffraction, Raman spectroscopy, scanning electron microscopy equipped with energy dispersive X-ray spectroscopy and X-ray photoelectron spectroscopy. It was found that the mass gain of the alloy in supercritical water decreased with increasing exposure time. The oxide films have a double-layer structure, with an inner layer rich in Cr and outer layer rich in Ni and Fe after short time and long time exposure. The penetration of the oxide along the grain boundaries was observed, and the penetration depth increased with increasing exposure time. The grain boundaries and voids are the short-path of oxygen diffusion into the metal. |
Other Abstract | The oxide films formed on Alloy 690 exposed to 600 ?C supercritical water were characterized using mass measurement, X-ray diffraction, Raman spectroscopy, scanning electron microscopy equipped with energy dispersive X-ray spectroscopy and X-ray photoelectron spectroscopy. It was found that the mass gain of the alloy in supercritical water decreased with increasing exposure time. The oxide films have a double-layer structure, with an inner layer rich in Cr and outer layer rich in Ni and Fe after short time and long time exposure. The penetration of the oxide along the grain boundaries was observed, and the penetration depth increased with increasing exposure time. The grain boundaries and voids are the short-path of oxygen diffusion into the metal. |
Keyword | Ni-based alloy XPS Supercritical water High temperature corrosion High temperature oxidation Oxide film |
Indexed By | CSCD |
Language | 英语 |
CSCD ID | CSCD:6216292 |
Citation statistics |
Cited Times:1[CSCD]
[CSCD Record]
|
Document Type | 期刊论文 |
Identifier | http://ir.imr.ac.cn/handle/321006/149820 |
Collection | 中国科学院金属研究所 |
Affiliation | 中国科学院金属研究所 |
Recommended Citation GB/T 7714 | Zhong Xiangyu,Wu Xinqiang,Han Enhou. Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 °C Aerated Supercritical Water[J]. Journal of Materials Science & Technology,2018,34(3):561-569. |
APA | Zhong Xiangyu,Wu Xinqiang,&Han Enhou.(2018).Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 °C Aerated Supercritical Water.Journal of Materials Science & Technology,34(3),561-569. |
MLA | Zhong Xiangyu,et al."Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 °C Aerated Supercritical Water".Journal of Materials Science & Technology 34.3(2018):561-569. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment