Al对GH4169合金冲击性能的影响 | |
其他题名 | Effect of Al on impact strength of GH4169 alloy |
刘芳1; 孙文儒2; 杨树林2; 赵长虹3; 魏志坚4; 郭守仁2; 杨洪才1; 胡壮麒2 | |
2008 | |
发表期刊 | 材料研究学报
![]() |
ISSN | 1005-3093 |
卷号 | 22.0期号:003页码:230-234 |
摘要 | 研究了Al对GH4169合金晶界相的析出和冲击性能的影响.结果表明,提高Al含量可抑制晶界δ相的析出,促进晶界Laves相、M7C3相和σ相等有害相的析出;随着Al含量的提高,GH4169合金的室温冲击性能明显降低,冲击断口由穿晶型转变为沿晶型.提高Al含量所导致的Laves相等有害脆性相的析出降低了晶界强度,使晶界裂纹更容易萌生和扩展,降低了GH4169合金的冲击韧性. |
其他摘要 | The effect of AI on the grain boundary precipitation and impact toughness of GH4169 alloy was investigated. The delta phase precipitation at the grain boundaries is noticeably suppressed due to the increasing Al addition, and some harmful phases including Laves phase, M7C3 carbide and sigma phase are formed intergranularly. As a result, the ‘U' notch impact energy is largely decreased. The cracks incline to be initiated and propagated at the carbides and other harmful phases precipitated along the grain boundaries, and hence the fracture energy of the alloy with higher AI contents is reduced. |
关键词 | 金属材料 GH4169 Al M7C3碳化物 Laves相 σ相 沿晶断裂 |
收录类别 | CSCD |
语种 | 中文 |
CSCD记录号 | CSCD:3323499 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/156855 |
专题 | 中国科学院金属研究所 |
作者单位 | 1.东北大学 2.中国科学院金属研究所 3.东北特钢集团有限责任公司 4.贵州安大航空锻造有限责任公司 |
推荐引用方式 GB/T 7714 | 刘芳,孙文儒,杨树林,等. Al对GH4169合金冲击性能的影响[J]. 材料研究学报,2008,22.0(003):230-234. |
APA | 刘芳.,孙文儒.,杨树林.,赵长虹.,魏志坚.,...&胡壮麒.(2008).Al对GH4169合金冲击性能的影响.材料研究学报,22.0(003),230-234. |
MLA | 刘芳,et al."Al对GH4169合金冲击性能的影响".材料研究学报 22.0.003(2008):230-234. |
条目包含的文件 | 条目无相关文件。 |
个性服务 |
推荐该条目 |
保存到收藏夹 |
查看访问统计 |
导出为Endnote文件 |
谷歌学术 |
谷歌学术中相似的文章 |
[刘芳]的文章 |
[孙文儒]的文章 |
[杨树林]的文章 |
百度学术 |
百度学术中相似的文章 |
[刘芳]的文章 |
[孙文儒]的文章 |
[杨树林]的文章 |
必应学术 |
必应学术中相似的文章 |
[刘芳]的文章 |
[孙文儒]的文章 |
[杨树林]的文章 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论