Synergism between wear and corrosion of Cr26Mo1 ferrite stainless steels in 0.5 mol/L of sulfuric acid | |
Dai, Zhixin1,2,3; Jiang, Shengli1,2,3; Wu, Bi1,3; Ning, Likui1,2; Li, Shu1,2,3; Duan, Deli1,2,3 | |
Corresponding Author | Jiang, Shengli(sljiang@imr.ac.cn) ; Duan, Deli(duandl@imr.ac.cn) |
2023-02-01 | |
Source Publication | TRIBOLOGY INTERNATIONAL
![]() |
ISSN | 0301-679X |
Volume | 178Pages:15 |
Abstract | In this paper, the tribocorrosion behavior of an ultra-pure high-chromium ferrite stainless-steel Cr26Mo1 in a 0.5 mol/L H2SO4 solution was investigated. Results show that the slight damage caused by PEEK to Cr26Mo1 is mainly scratching, micro-furrow, and micro-peeling, while the severe damage caused by Al2O3 to Cr26Mo1 is mainly furrow, peeling, and plastic deformation. The deformed layer in the subsurface of the wear track is closely related to the shear stress applied to the material. Geometrically necessary dislocations and the rotation of crystals greatly contribute to the deformation. The microdefects on the surface and subsurface caused by wear may accelerate corrosion, and the decline of microhardness and H adsorption in the surface layer caused by corrosion could deteriorate wear. |
Keyword | Tribocorrosion Synergism Ferrite stainless steel Sulfuric acid |
DOI | 10.1016/j.triboint.2022.108007 |
Indexed By | SCI |
Language | 英语 |
WOS Research Area | Engineering |
WOS Subject | Engineering, Mechanical |
WOS ID | WOS:000884804300002 |
Publisher | ELSEVIER SCI LTD |
Citation statistics | |
Document Type | 期刊论文 |
Identifier | http://ir.imr.ac.cn/handle/321006/176717 |
Collection | 中国科学院金属研究所 |
Corresponding Author | Jiang, Shengli; Duan, Deli |
Affiliation | 1.Chinese Acad Sci, Inst Met Res, Shi Changxu Innovat Ctr Adv Mat, 72 Wenhua Rd, Shenyang 110016, Peoples R China 2.Univ Sci & Technol China, Sch Mat Sci & Engn, 96 Jinzhai Rd, Hefei 230026, Peoples R China 3.Chinese Acad Sci, Inst Met Res, Liaoning Key Lab Aeroengine Mat Tribol, 72 Wenhua Rd, Shenyang 110016, Peoples R China |
Recommended Citation GB/T 7714 | Dai, Zhixin,Jiang, Shengli,Wu, Bi,et al. Synergism between wear and corrosion of Cr26Mo1 ferrite stainless steels in 0.5 mol/L of sulfuric acid[J]. TRIBOLOGY INTERNATIONAL,2023,178:15. |
APA | Dai, Zhixin,Jiang, Shengli,Wu, Bi,Ning, Likui,Li, Shu,&Duan, Deli.(2023).Synergism between wear and corrosion of Cr26Mo1 ferrite stainless steels in 0.5 mol/L of sulfuric acid.TRIBOLOGY INTERNATIONAL,178,15. |
MLA | Dai, Zhixin,et al."Synergism between wear and corrosion of Cr26Mo1 ferrite stainless steels in 0.5 mol/L of sulfuric acid".TRIBOLOGY INTERNATIONAL 178(2023):15. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment