Effect of temperature on the delayed hydride cracking rate of Zr-2.5Nb alloy pressure tubes
Pan, Chunting1,2; Zhao, Guannan3; Bao, Yichen3; Zhang, Zhiming2,4; Shi, Xiuqiang3; Meng, Fanjiang3; Wang, Jianqiu1,2,4; Ming, Hongliang1,2
Corresponding AuthorZhang, Zhiming(zmzhang@icost.ac.cn) ; Ming, Hongliang(hlming12s@imr.ac.cn)
2024
Source PublicationJOURNAL OF NUCLEAR MATERIALS
ISSN0022-3115
Volume588Pages:10
AbstractDelayed hydride cracking (DHC) is a potential failure mechanism of Zr-2.5Nb alloy pressure tubes, employed in heavy-water reactors. This study focused on understanding the DHC behavior of the Zr-2.5Nb pressure tubes within the temperature range 393-523 K. Our findings demonstrate that within this temperature range, the delayed hydride cracking rate (DHCR) and temperature follow the Arrhenius relationship, with the activation energy of crack propagation is found to be 43.16 kJ/mol. The changes in the fracture morphologies at different temperatures are analyzed. Variations in the fracture hydride lengths with temperature and the stress intensity factor K are obtained. Furthermore, it is found that the influencing mechanism of temperature on DHC behavior changes as the temperature increases.
KeywordDelayed hydride cracking Zr-2.5Nb alloy Heavy water reactor
Funding OrganizationYouth Innovation Promotion Assess- ment CAS
DOI10.1016/j.jnucmat.2023.154778
Indexed BySCI
Language英语
Funding ProjectYouth Innovation Promotion Assess- ment CAS[2022187]
WOS Research AreaMaterials Science ; Nuclear Science & Technology
WOS SubjectMaterials Science, Multidisciplinary ; Nuclear Science & Technology
WOS IDWOS:001105362300001
PublisherELSEVIER
Citation statistics
Cited Times:5[WOS]   [WOS Record]     [Related Records in WOS]
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/177355
Collection中国科学院金属研究所
Corresponding AuthorZhang, Zhiming; Ming, Hongliang
Affiliation1.Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Peoples R China
2.Chinese Acad Sci, Key Lab Nucl Mat & Safety Assessment, Inst Met Res, Shenyang 110016, Peoples R China
3.Shanghai Nucl Engn Res & Design Inst Ltd Co, Shanghai 200233, Peoples R China
4.Inst Corros Sci & Technol, Guangzhou 510530, Peoples R China
Recommended Citation
GB/T 7714
Pan, Chunting,Zhao, Guannan,Bao, Yichen,et al. Effect of temperature on the delayed hydride cracking rate of Zr-2.5Nb alloy pressure tubes[J]. JOURNAL OF NUCLEAR MATERIALS,2024,588:10.
APA Pan, Chunting.,Zhao, Guannan.,Bao, Yichen.,Zhang, Zhiming.,Shi, Xiuqiang.,...&Ming, Hongliang.(2024).Effect of temperature on the delayed hydride cracking rate of Zr-2.5Nb alloy pressure tubes.JOURNAL OF NUCLEAR MATERIALS,588,10.
MLA Pan, Chunting,et al."Effect of temperature on the delayed hydride cracking rate of Zr-2.5Nb alloy pressure tubes".JOURNAL OF NUCLEAR MATERIALS 588(2024):10.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[Pan, Chunting]'s Articles
[Zhao, Guannan]'s Articles
[Bao, Yichen]'s Articles
Baidu academic
Similar articles in Baidu academic
[Pan, Chunting]'s Articles
[Zhao, Guannan]'s Articles
[Bao, Yichen]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[Pan, Chunting]'s Articles
[Zhao, Guannan]'s Articles
[Bao, Yichen]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.