Hot corrosion behaviors of 921A alloy and HVAF-sprayed Fe-based amorphous coating covered with KCl-ZnCl2 salts
Zhang, Hai-liang1,2; Yang, Ling-xu3; Wang, Qian4; Wu, Jiang-tao1,2; Zhang, Suo-de1; Zeng, Chao-liu3
通讯作者Zhang, Suo-de(sdzhang@imr.ac.cn) ; Zeng, Chao-liu(clzeng@imr.ac.cn)
2023-07-04
发表期刊JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL
ISSN1006-706X
页码13
摘要Hot corrosion behaviors of the 921A alloy and Fe-based amorphous coating induced by KCl-10% ZnCl2 and KCl-55% ZnCl2 salts at 450 & DEG;C in air for 40 h were investigated. Results show that the 921A alloy suffers more serious corrosion damage than the coating and KCl-55% ZnCl2 salts are more corrosive than KCl-10% ZnCl2 salts. In the two salts, an Fe2O3 layer is formed on the 921A alloy surface, while an outer Fe-rich oxide layer and an inner Cr-rich oxide layer are formed on the surface of the coating. Moreover, a certain amount of metal chloride can be found at the oxide/alloy (coating) interface, which can be explained by "active oxidation". However, the corrosion resistance of the Fe-based amorphous coating did not achieve the desired results, probably because the intersplats in the coating serve as corrosion diffusing channels, which facilitate the corrosion damage rate. Nevertheless, the coating is still in amorphous state after hot corrosion exposure.
关键词Hot corrosion Chloride deposit 921A alloy Fe-based amorphous coating Waste-to-energy plant
资助者GuangDong Basic and Applied Basic Research Foundation
DOI10.1007/s42243-023-01011-6
收录类别SCI
语种英语
资助项目GuangDong Basic and Applied Basic Research Foundation[2020A1515110128]
WOS研究方向Metallurgy & Metallurgical Engineering
WOS类目Metallurgy & Metallurgical Engineering
WOS记录号WOS:001022477300001
出版者SPRINGER
引用统计
被引频次:1[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/178517
专题中国科学院金属研究所
通讯作者Zhang, Suo-de; Zeng, Chao-liu
作者单位1.Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China
2.Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Liaoning, Peoples R China
3.Songshan Lake Mat Lab, Dongguan 523808, Guangdong, Peoples R China
4.Univ Sci & Technol Liaoning, Sch Mat & Met, Anshan 114051, Liaoning, Peoples R China
推荐引用方式
GB/T 7714
Zhang, Hai-liang,Yang, Ling-xu,Wang, Qian,et al. Hot corrosion behaviors of 921A alloy and HVAF-sprayed Fe-based amorphous coating covered with KCl-ZnCl2 salts[J]. JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL,2023:13.
APA Zhang, Hai-liang,Yang, Ling-xu,Wang, Qian,Wu, Jiang-tao,Zhang, Suo-de,&Zeng, Chao-liu.(2023).Hot corrosion behaviors of 921A alloy and HVAF-sprayed Fe-based amorphous coating covered with KCl-ZnCl2 salts.JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL,13.
MLA Zhang, Hai-liang,et al."Hot corrosion behaviors of 921A alloy and HVAF-sprayed Fe-based amorphous coating covered with KCl-ZnCl2 salts".JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL (2023):13.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Zhang, Hai-liang]的文章
[Yang, Ling-xu]的文章
[Wang, Qian]的文章
百度学术
百度学术中相似的文章
[Zhang, Hai-liang]的文章
[Yang, Ling-xu]的文章
[Wang, Qian]的文章
必应学术
必应学术中相似的文章
[Zhang, Hai-liang]的文章
[Yang, Ling-xu]的文章
[Wang, Qian]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。