Four-point method in evaluating the corrosion rate of secondary circuit structural materials in nuclear power plant | |
Ji, Yuefei1,2; Hao, Long1,2; Wang, Jianqiu1,3; Han, En-Hou1,3; Ke, Wei1 | |
通讯作者 | Hao, Long(lhao@imr.ac.cn) |
2024-11-18 | |
发表期刊 | ANTI-CORROSION METHODS AND MATERIALS
![]() |
ISSN | 0003-5599 |
页码 | 11 |
摘要 | Purpose - The purpose of this paper is to optimize a suitable electrochemical method in evaluating the corrosion rate of structural materials of 20# carbon steel, P280GH carbon steel, 17-4PH stainless steel, 304 stainless steel and Alloy 690TT in high-temperature and high-pressure (HTHP) water of pressurized water reactor secondary circuit system. Design/methodology/approach - Weight-loss method has been used to obtain the corrosion rate value of each structural material in simulated HTHP water. Besides, linear polarization method and weak polarization curve-based three-point method and four-point method have been compared in obtaining a sound corrosion rate value from the potentiodynamic polarization curve. Scanning electron microscopy (SEM) and atomic force microscope have been used to characterize the microstructure and corrosion morphology of each structural material. Findings - Although there is deviation in gaining the corrosion rate value compared to weight-loss test, the weak polarization curve-based four- point method has been found to be a suitable electrochemical method in gaining corrosion rate value of structural materials in HTHP waters. Originality/value - This paper proposes a suitable and reliable electrochemical method in gaining the corrosion rate value of structural materials in HTHP waters. The proposed weak polarization curve-based four-point method provides a timesaving and high-efficient way in corrosion rate evaluation of secondary circuit structural materials and thus has a potential application in nuclear power plants. |
关键词 | Alkalizer Uniform corrosion High-temperature electrochemistry Secondary circuit |
资助者 | LingChuang Research Project of China National Nuclear Corporation |
DOI | 10.1108/ACMM-09-2024-3091 |
收录类别 | SCI |
语种 | 英语 |
资助项目 | LingChuang Research Project of China National Nuclear Corporation |
WOS研究方向 | Metallurgy & Metallurgical Engineering |
WOS类目 | Metallurgy & Metallurgical Engineering |
WOS记录号 | WOS:001354592800001 |
出版者 | EMERALD GROUP PUBLISHING LTD |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/191394 |
专题 | 中国科学院金属研究所 |
通讯作者 | Hao, Long |
作者单位 | 1.Chinese Acad Sci, CAS Key Lab Nucl Mat & Safety Assessment, Inst Met Res, Shenyang, Peoples R China 2.Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang, Peoples R China 3.Inst Corros Sci & Technol, Guangzhou, Peoples R China |
推荐引用方式 GB/T 7714 | Ji, Yuefei,Hao, Long,Wang, Jianqiu,et al. Four-point method in evaluating the corrosion rate of secondary circuit structural materials in nuclear power plant[J]. ANTI-CORROSION METHODS AND MATERIALS,2024:11. |
APA | Ji, Yuefei,Hao, Long,Wang, Jianqiu,Han, En-Hou,&Ke, Wei.(2024).Four-point method in evaluating the corrosion rate of secondary circuit structural materials in nuclear power plant.ANTI-CORROSION METHODS AND MATERIALS,11. |
MLA | Ji, Yuefei,et al."Four-point method in evaluating the corrosion rate of secondary circuit structural materials in nuclear power plant".ANTI-CORROSION METHODS AND MATERIALS (2024):11. |
条目包含的文件 | 条目无相关文件。 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论