Fatigue deformation characteristic of as-extruded AM30 magnesium alloy | |
T. J. Luo; Y. S. Yang; W. H. Tong; Q. Q. Duan; X. G. Dong | |
2010 | |
发表期刊 | Materials & Design
![]() |
ISSN | 0261-3069 |
卷号 | 31期号:3页码:1617-1621 |
摘要 | The fatigue deformation behavior of as-extruded AM30 magnesium alloy has been investigated under different strain amplitudes in this paper, and the microstructure and fractograph during the cyclic deformation have been analyzed by use of the optical microscope (OM) and the scanning electronic microscope (SEM). The results show that there are many {10-12} twins in the fatigue specimens of the extruded AM30 alloy, and with the increase of total strain amplitude, the twins become coarser and longer. Otherwise, there are many twin bands composed of many tiny lenticular type twins ({10-12}< 10-11 > twin) near the fatigue fracture, which become more with increase of total strain amplitude. (C) 2009 Elsevier Ltd. All rights reserved. |
部门归属 | [luo, t. j.; yang, y. s.; tong, w. h.; duan, q. q.; dong, x. g.] chinese acad sci, inst met res, shenyang 110016, peoples r china.;yang, ys (reprint author), chinese acad sci, inst met res, shenyang 110016, peoples r china;ysyang@imr.ac.cn |
关键词 | Az31 Mg Alloy Behavior Temperature Mechanisms |
URL | 查看原文 |
WOS记录号 | WOS:000274203200076 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/31359 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | T. J. Luo,Y. S. Yang,W. H. Tong,et al. Fatigue deformation characteristic of as-extruded AM30 magnesium alloy[J]. Materials & Design,2010,31(3):1617-1621. |
APA | T. J. Luo,Y. S. Yang,W. H. Tong,Q. Q. Duan,&X. G. Dong.(2010).Fatigue deformation characteristic of as-extruded AM30 magnesium alloy.Materials & Design,31(3),1617-1621. |
MLA | T. J. Luo,et al."Fatigue deformation characteristic of as-extruded AM30 magnesium alloy".Materials & Design 31.3(2010):1617-1621. |