Mechanisms and Kinetics of the Hydrothermal Oxidation of Bulk Titanium Silicon Carbide | |
H. B. Zhang; V. Presser; C. Berthold; K. G. Nickel; X. Wang; C. Raisch; T. Chasse; L. F. He; Y. C. Zhou | |
2010 | |
发表期刊 | Journal of the American Ceramic Society
![]() |
ISSN | 0002-7820 |
卷号 | 93期号:4页码:1148-1155 |
摘要 | Hydrothermal oxidation of bulk Ti(3)SiC(2) in continuous water flow was studied at 500 degrees-700 degrees C under a hydrostatic pressure of 35 MPa. The oxidation was weak at 500 degrees-600 degrees C and accelerated at 700 degrees C due to the formation of cracks in oxides. The kinetics obeyed a linear time-law. Due to the high solubility of silica in hydrothermal water, the resulting oxide layers only consisted of titanium oxides and carbon. Besides general oxidation, two special modes are very likely present in current experiments: (1) preferential hydrothermal oxidation of lattice planes perpendicular to the c-axis inducing cleavage of grains and (2) uneven hydrothermal oxidation related to the occurrence of TiC and SiC impurity inclusions. Nonetheless the resistance against hydrothermal oxidation is remarkably high up to 700 degrees C. |
部门归属 | [zhang, haibin; presser, volker; berthold, christoph; nickel, klaus georg; wang, xin] univ tubingen, inst geosci, d-72074 tubingen, germany. [raisch, christoph; chasse, thomas] univ tubingen, inst phys & theoret chem, d-72076 tubingen, germany. [he, lingfeng; zhou, yanchun] chinese acad sci, inst met res, shenyang natl lab mat sci, shenyang 110016, peoples r china.;zhang, hb (reprint author), univ tubingen, inst geosci, wilhelmstr 56, d-72074 tubingen, germany;hbzhang1978@gmail.com |
关键词 | Amorphous-carbon Films Ti3si0.9al0.1c2 Solid-solution Temperature Oxidation m(n+1)Ax(n) Phases Ternary Carbides Ti3sic2 Powders Laser Raman Thin-film Behavior Corrosion |
URL | 查看原文 |
WOS记录号 | WOS:000276246700044 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/31691 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | H. B. Zhang,V. Presser,C. Berthold,et al. Mechanisms and Kinetics of the Hydrothermal Oxidation of Bulk Titanium Silicon Carbide[J]. Journal of the American Ceramic Society,2010,93(4):1148-1155. |
APA | H. B. Zhang.,V. Presser.,C. Berthold.,K. G. Nickel.,X. Wang.,...&Y. C. Zhou.(2010).Mechanisms and Kinetics of the Hydrothermal Oxidation of Bulk Titanium Silicon Carbide.Journal of the American Ceramic Society,93(4),1148-1155. |
MLA | H. B. Zhang,et al."Mechanisms and Kinetics of the Hydrothermal Oxidation of Bulk Titanium Silicon Carbide".Journal of the American Ceramic Society 93.4(2010):1148-1155. |