IMR OpenIR
Helium Retention and Desorption Behaviour of Reduced Activation Ferritic/Martenstic Steel
P. H. Wang; Y. Nobuta; T. Hino; Y. Yamauchi; J. M. Chen; Z. Y. Xu; X. W. Li; S. Liu
2009
发表期刊Plasma Science & Technology
ISSN1009-0630
卷号11期号:2页码:225-230
摘要The reduced activation ferritic/martenstic steel CLF-1 prepared by the Southwestern Institute of Physics in China was irradiated by helium ions with an energy of 5 keV at room temperature using an electron cyclotron resonance (ECR) ion irradiation apparatus. After the irradiation, the helium retention and desorption were investigated using a technique of thermal desorption spectroscopy (TDS). The experiment was conducted with both the normal and welded samples. Blisters were observed after the helium ion irradiation, and the surface density of blisters in the welded samples was lower than that in the non-welded samples. Three desorption peaks were observed in both the non-welded and welded samples. These desorption peaks corresponded to those of blister ruptures and the helium release from the inner bubbles and the defects. The amount of helium retained in the welded samples was approximately the same as that in the non-welded samples, which was much less than other reduced activation materials, such as vanadium alloy and SiC/SiC composites.
部门归属[wang pinghuai; yamauchi yuji; chen jiming; xu zengyu] sw inst phys, chengdu 610041, peoples r china. [nobuta yuji; hino tomoaki] hokkaido univ, lab plasma phys & engn, sapporo, hokkaido 0608628, japan. [li xiongwei; liu shi] chinese acad sci, inst met res, shenyang 110016, peoples r china.;wang, ph (reprint author), sw inst phys, chengdu 610041, peoples r china;wangph@swip.ac.cn
关键词Reduced Activation Material Helium Ion irradiatIon Helium Retention Fusion Reactor Ferritic Steels Alloy
URL查看原文
WOS记录号WOS:000264950900018
引用统计
被引频次:10[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/32368
专题中国科学院金属研究所
推荐引用方式
GB/T 7714
P. H. Wang,Y. Nobuta,T. Hino,et al. Helium Retention and Desorption Behaviour of Reduced Activation Ferritic/Martenstic Steel[J]. Plasma Science & Technology,2009,11(2):225-230.
APA P. H. Wang.,Y. Nobuta.,T. Hino.,Y. Yamauchi.,J. M. Chen.,...&S. Liu.(2009).Helium Retention and Desorption Behaviour of Reduced Activation Ferritic/Martenstic Steel.Plasma Science & Technology,11(2),225-230.
MLA P. H. Wang,et al."Helium Retention and Desorption Behaviour of Reduced Activation Ferritic/Martenstic Steel".Plasma Science & Technology 11.2(2009):225-230.
条目包含的文件
文件名称/大小 文献类型 版本类型 开放类型 使用许可
2136.pdf(773KB) 开放获取--
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[P. H. Wang]的文章
[Y. Nobuta]的文章
[T. Hino]的文章
百度学术
百度学术中相似的文章
[P. H. Wang]的文章
[Y. Nobuta]的文章
[T. Hino]的文章
必应学术
必应学术中相似的文章
[P. H. Wang]的文章
[Y. Nobuta]的文章
[T. Hino]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。