Air corrosion of Fe-15Cr-xAl alloys beneath KCl-ZnCl2 deposits at 773K | |
T. J. Pan; W. T. Wu; C. L. Zeng; Y. Niu | |
2006 | |
发表期刊 | High Temperature Materials and Processes
![]() |
ISSN | 0334-6455 |
卷号 | 25期号:5-6页码:255-260 |
摘要 | The corrosion behavior of three Fe-15Cr-xAl alloys (x=0, 5, 10 at.%) beneath KCl-ZnCl2 deposits in air was investigated at 773K. All the alloys suffered from accelerated corrosion characterized by the formation of non-protective porous oxide scales. The addition of aluminum was only slightly beneficial for the corrosion resistance of the base alloy. The effect of aluminum is attributed to the increase of the Al2O3 content in the inner region of the scale, which may act as a barrier by retarding the rapid migration of the reactants. |
部门归属 | chinese acad sci, met res inst, state key lab corros & protect, shenyang 110016, peoples r china.;niu, y (reprint author), chinese acad sci, met res inst, state key lab corros & protect, wencui rd 62, shenyang 110016, peoples r china, peoples r china;yniu@imr.ac.cn |
关键词 | Fe-cr-al Al Effect Kcl-zncl2 Chlorination High-temperature Corrosion Waste Incineration Environment Stainless-steels Cr Fe Oxidation Zncl2-kcl Behavior Elements Melt |
URL | 查看原文 |
WOS记录号 | WOS:000244099100002 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/34417 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | T. J. Pan,W. T. Wu,C. L. Zeng,et al. Air corrosion of Fe-15Cr-xAl alloys beneath KCl-ZnCl2 deposits at 773K[J]. High Temperature Materials and Processes,2006,25(5-6):255-260. |
APA | T. J. Pan,W. T. Wu,C. L. Zeng,&Y. Niu.(2006).Air corrosion of Fe-15Cr-xAl alloys beneath KCl-ZnCl2 deposits at 773K.High Temperature Materials and Processes,25(5-6),255-260. |
MLA | T. J. Pan,et al."Air corrosion of Fe-15Cr-xAl alloys beneath KCl-ZnCl2 deposits at 773K".High Temperature Materials and Processes 25.5-6(2006):255-260. |
条目包含的文件 | 条目无相关文件。 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论