Oxidation behavior of ternary Fe-15Cu-5Al and Fe-85Cu-5Al alloys in pure oxygen at 900 degrees C | |
J. H. Xiang; Y. Niu; X. Z. Duan | |
2006 | |
发表期刊 | Transactions of Nonferrous Metals Society of China
![]() |
ISSN | 1003-6326 |
卷号 | 16页码:S2038-S2041 |
摘要 | The oxidation of two two-phase ternary Fe-Cu-Al alloys containing about 5%(mole fraction) aluminium, one Fe-rich and one Cu-rich, has been studied at 900 degrees C in 1 x 10(5) pa pure oxygen. The Fe-rich Fe-15Cu-5Al alloy presents two quasi-parabolic stages, with a large decrease of the parabolic rate constant after about 50 min. The presence of 5% At greatly reduces the oxidation rate of this alloy with respect to a binary Fe-Cu alloy of similar composition by forming an external protective Al2O3 layer, which is present near the scale/alloy interface. Due to the high stress-growth effect, this thin Al2O3 layer cannot completely prevent further oxidation of the alloy underneath. On the contrary, the Cu-rich Fc-85Cu-5Al alloy presents a single parabolic stage and forms a thick and porous external scale, coupled to the internal oxidation of Fe and Al. As a result, the oxidation of Cu-rich alloy at 900 degrees C is much faster than that of the Fe-rich alloy. |
部门归属 | jiangxi sci & technol normal univ, jiangxi key lab surface engn, nanchang 330013, peoples r china. chinese acad sci, met res inst, state key lab corros & protect, shenyang 110016, peoples r china. xiangtan univ, key lab minist educ low dimens mat & appl technol, xiangtan 411105, peoples r china.;xiang, jh (reprint author), jiangxi sci & technol normal univ, jiangxi key lab surface engn, nanchang 330013, peoples r china;xiangjunhuai@163.com |
关键词 | Fe-15cu-5al Alloy Fe-85cu-5al Alloy Ternary Alloy Oxidation Behavior At.percent-al-alloys Forming Insoluble Oxides External Oxidation 1 Atm Approximate Analysis Oxidant Pressures Air Oxidation O-2 800-900-degrees-c |
URL | 查看原文 |
WOS记录号 | WOS:000244524400182 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/34588 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | J. H. Xiang,Y. Niu,X. Z. Duan. Oxidation behavior of ternary Fe-15Cu-5Al and Fe-85Cu-5Al alloys in pure oxygen at 900 degrees C[J]. Transactions of Nonferrous Metals Society of China,2006,16:S2038-S2041. |
APA | J. H. Xiang,Y. Niu,&X. Z. Duan.(2006).Oxidation behavior of ternary Fe-15Cu-5Al and Fe-85Cu-5Al alloys in pure oxygen at 900 degrees C.Transactions of Nonferrous Metals Society of China,16,S2038-S2041. |