The oxidation of four Ni-xSi-6Al alloys (x = 0, 2,4 and 6 at.%) has been studied at 1273 K under 0.1 MPa O-2. Silicon exerts the third-element effect by reducing the critical Al content needed for the transition from its internal to its external oxidation with respect to Ni-Al alloys. This result is interpreted by extending to ternary alloys Wagner's criterion for the same transition in binary alloys. (c) 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
部门归属
chinese acad sci, state key lab corros & protect, inst met res, shenyang 110016, peoples r china.;niu, y (reprint author), chinese acad sci, state key lab corros & protect, inst met res, wencui rd 62, shenyang 110016, peoples r china;ywu@imr.ac.cn yniu@imr.ac.cn