Atmospheric corrosion of A3 steel deposited with different salts | |
Y. Wan; C. W. Yan; C. N. Cao | |
2004 | |
发表期刊 | Acta Physico-Chimica Sinica
![]() |
ISSN | 1000-6818 |
卷号 | 20期号:6页码:659-663 |
摘要 | The atmospheric corrosion of A3 steel with Na2SO4,(NH4) SO4,NH4Cl and NaCl deposited on it has been investigated at 298 K with relative humidity of (85 +/- 5) %. The results show: that A3 steel deposited by the salts corroded more and more seriously as the corrosion time went on and metal loss obeys the equation of Deltam/ A = K . t(h). FTIR, SEM and XRD were utilized to study the development and characterization of corrosion products, and the results indicate that A3 steel with the salts deposited corroded much faster than the blank samples, and the corrosion of A3 steel initialed along the deposition area of the salts. |
部门归属 | chinese acad sci, inst met res, state key lab corros & protect, shenyang 110016, peoples r china.;wan, y (reprint author), chinese acad sci, inst met res, state key lab corros & protect, shenyang 110016, peoples r china;ywan@imr.ac.cn |
关键词 | Steel A3 Salt Deposition Atmospheric Corrosion Ammonium-sulfate Zinc Products Rust Nacl |
URL | 查看原文 |
WOS记录号 | WOS:000222223400022 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/35570 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | Y. Wan,C. W. Yan,C. N. Cao. Atmospheric corrosion of A3 steel deposited with different salts[J]. Acta Physico-Chimica Sinica,2004,20(6):659-663. |
APA | Y. Wan,C. W. Yan,&C. N. Cao.(2004).Atmospheric corrosion of A3 steel deposited with different salts.Acta Physico-Chimica Sinica,20(6),659-663. |
MLA | Y. Wan,et al."Atmospheric corrosion of A3 steel deposited with different salts".Acta Physico-Chimica Sinica 20.6(2004):659-663. |