IMR OpenIR
The corrosion of various materials under chloride deposits at 623-723K in pure oxygen
Y. S. Li; M. Al-Omary; Y. Niu; K. Zhang
2002
发表期刊High Temperature Materials and Processes
ISSN0334-6455
卷号21期号:1-2页码:41237
摘要Corrosion problems in waste incinerators or in other advanced combustion power generation systems are usually rather serious due to the deposition of ashes composed of heavy and alkali metal chlorides or sulfates of metals such as Zn, K, Pb etc. This paper presents the individual and combined effects of ZnCl2 and KCl on the corrosion behavior of some heat-resistant steels, the M38G Ni-based alloy, 2205 duplex steel and several other Fe-based alloys as well as pure metals were examined at 623K and 723K in pure oxygen. All the materials tested suffered from accelerated corrosion due to the formation of non-protective porous oxide scales and in many cases from local attack in the alloy matrix induced by chlorine. The Cr addition to the alloys can hardly provide sufficient corrosion resistance against such environments as a result of the bad adherence of Cr2O3 to the alloy matrix. This detrimental effect is discussed on the basis of thermodynamic considerations.
部门归属inst met sci & technol, state key lab corros & protect, shenyang 110016, peoples r china. univ sharjah, dept basic sci, sharjah, u arab emirates.;niu, y (reprint author), inst met sci & technol, state key lab corros & protect, south campus,wencui rd 63, shenyang 110016, peoples r china
关键词Chloride Deposits Corrosion Alloys Waste Incineration Stainless-steels Molten Chlorides Hot Corrosion Environments Behavior
URL查看原文
WOS记录号WOS:000176799900002
引用统计
被引频次:14[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/36324
专题中国科学院金属研究所
推荐引用方式
GB/T 7714
Y. S. Li,M. Al-Omary,Y. Niu,et al. The corrosion of various materials under chloride deposits at 623-723K in pure oxygen[J]. High Temperature Materials and Processes,2002,21(1-2):41237.
APA Y. S. Li,M. Al-Omary,Y. Niu,&K. Zhang.(2002).The corrosion of various materials under chloride deposits at 623-723K in pure oxygen.High Temperature Materials and Processes,21(1-2),41237.
MLA Y. S. Li,et al."The corrosion of various materials under chloride deposits at 623-723K in pure oxygen".High Temperature Materials and Processes 21.1-2(2002):41237.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Y. S. Li]的文章
[M. Al-Omary]的文章
[Y. Niu]的文章
百度学术
百度学术中相似的文章
[Y. S. Li]的文章
[M. Al-Omary]的文章
[Y. Niu]的文章
必应学术
必应学术中相似的文章
[Y. S. Li]的文章
[M. Al-Omary]的文章
[Y. Niu]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。