Low cycle fatigue in titanium aluminium formed by centrifugal spray deposition | |
W. Z. Chen; S. Zhang; K. W. Qian; H. C. Gu; Z. G. Wang | |
1998 | |
发表期刊 | Transactions of Nonferrous Metals Society of China
![]() |
ISSN | 1003-6326 |
卷号 | 8期号:2页码:240-244 |
摘要 | The push-pull low cycle fatigue (LCF) behaviors of Ti-48Al-2Mn-2Nb (mole fraction, %), which was formed by centrifugal spray deposition (CSD) under a low pressure vacuum condition, were investigated under the control of total cyclic strain amplitude at ambient temperature. The results show that the available cyclic strain amplitude regions of TiAl alloy are very narrow, Delta epsilon(tau)/2 equals 0.1% similar to 0.25 %, and no cyclic hardening or softening are observed during low cycle fatigue processes. The fatigue lives of CSD samples can be improved by hot isostatic pressing (HIP). The characteristics of dislocation configurations of samples experienced different strain amplitudes have been analyzed by means of transmission electron microscopy (TEM). |
部门归属 | fuzhou univ, dept mat, fuzhou 350002, peoples r china. xian jiao tong univ, sch mat sci & engn, xian 710049, peoples r china. acad sinica, inst met res, state key lab fatigue & fracture mat, shenyang 110015, peoples r china. |
关键词 | Centrifugal Spray Deposition (Csd) Ti-48al-2mn-2nb Low Cycle Fatigue Intermetallic Alloys |
URL | 查看原文 |
WOS记录号 | WOS:000074309300012 |
引用统计 | |
文献类型 | 期刊论文 |
条目标识符 | http://ir.imr.ac.cn/handle/321006/37640 |
专题 | 中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | W. Z. Chen,S. Zhang,K. W. Qian,et al. Low cycle fatigue in titanium aluminium formed by centrifugal spray deposition[J]. Transactions of Nonferrous Metals Society of China,1998,8(2):240-244. |
APA | W. Z. Chen,S. Zhang,K. W. Qian,H. C. Gu,&Z. G. Wang.(1998).Low cycle fatigue in titanium aluminium formed by centrifugal spray deposition.Transactions of Nonferrous Metals Society of China,8(2),240-244. |
MLA | W. Z. Chen,et al."Low cycle fatigue in titanium aluminium formed by centrifugal spray deposition".Transactions of Nonferrous Metals Society of China 8.2(1998):240-244. |