Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method
J. F. Hong; D. Han; H. Tan; J. Li; Y. M. Jiang
2013
发表期刊Corrosion Science
ISSN0010-938X
卷号68页码:249-255
摘要Optimized double loop electrochemical potentiokinetic reactivation (DL-EPR) in combination with microstructure observation were successfully applied to study the sensitization of super duplex stainless steel UNS S32750 aged at 900 degrees C for different duration to intergranular corrosion (IGC). The results indicated that the degree of sensitization increased gradually with the aging time increased from 10 min to 4 h due to the sigma phase precipitation, and I-r:I-a value reached the maximum value of 17.1%. However, further increasing aging time slightly decreased the sensitization due to the healing effect incurred by the diffusion of chromium from adjacent grains to chromium-depleted zone. (C) 2012 Elsevier Ltd. All rights reserved.
部门归属[hong, jufeng ; han, dong ; tan, hua ; li, jin ; jiang, yiming] fudan univ, dept mat sci, shanghai 200433, peoples r china. [tan, hua] state nucl power plant serv co, shanghai, peoples r china. [li, jin] chinese acad sci, inst met res, beijing 100864, peoples r china. ; jiang, ym (reprint author), fudan univ, dept mat sci, shanghai 200433, peoples r china. ; ymjiang@fudan.edu.cn
关键词Stainless Steel Sem Intergranular Corrosion Sensitization Resistance Unss31803 Behavior Environments Tests
URL查看原文
语种英语
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/71258
专题中国科学院金属研究所
推荐引用方式
GB/T 7714
J. F. Hong,D. Han,H. Tan,et al. Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method[J]. Corrosion Science,2013,68:249-255.
APA J. F. Hong,D. Han,H. Tan,J. Li,&Y. M. Jiang.(2013).Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method.Corrosion Science,68,249-255.
MLA J. F. Hong,et al."Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method".Corrosion Science 68(2013):249-255.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[J. F. Hong]的文章
[D. Han]的文章
[H. Tan]的文章
百度学术
百度学术中相似的文章
[J. F. Hong]的文章
[D. Han]的文章
[H. Tan]的文章
必应学术
必应学术中相似的文章
[J. F. Hong]的文章
[D. Han]的文章
[H. Tan]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。