High temperature thermo-mechanical and low cycle fatigue behaviors of DD32 single crystal superalloy
J. J. Yu; G. M. Han; Z. K. Chu; X. F. Sun; T. Jin; Z. Q. Hu
2014
Source PublicationMaterials Science and Engineering a-Structural Materials Properties Microstructure and Processing
ISSN0921-5093
Volume592Pages:164-172
AbstractFatigue cycles decrease in the sequence of in-phase TMF (IF), isothermal low cycle fatigue (IF), out-of-phase TMF (OP) in the temperature ranges from 600 degrees C to 900 degrees C when the total strain amplitude is taken as the basis. However, fatigue life decreases in the sequence of IF, OP, and IP with the mechanical strain range as the basis. At lower strain amplitude, the fracture surfaces of OP present a mass of typical fatigue steps. Nevertheless, at higher strain amplitude in IP case the fracture surfaces with a lot of planar dimples are similar to those of high temperature creep test. The common deformation features of IP, OP, and IF are a network of dislocations at lower strains and well defined dislocation bands at higher strains. (C) 2013 Elsevier B.V. All rights reserved.
description.department[yu, jinjiang ; han, guoming ; chu, zhaokuang ; sun, xiaofeng ; jin, tao ; hu, zhuangqi] chinese acad sci, inst met res, shenyang 110016, peoples r china. ; yu, jj (reprint author), chinese acad sci, inst met res, 72 wenhua rd, shenyang 110016, peoples r china. ; jjyu@imr.ac.cn
KeywordSingle Crystal Superalloy Thermo-mechanical Fatigue Deformation Mechanism Ni-base Superalloy Deformation Microstructure Failure Tms-75 Life
URL查看原文
Language英语
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/72505
Collection中国科学院金属研究所
Recommended Citation
GB/T 7714
J. J. Yu,G. M. Han,Z. K. Chu,et al. High temperature thermo-mechanical and low cycle fatigue behaviors of DD32 single crystal superalloy[J]. Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing,2014,592:164-172.
APA J. J. Yu,G. M. Han,Z. K. Chu,X. F. Sun,T. Jin,&Z. Q. Hu.(2014).High temperature thermo-mechanical and low cycle fatigue behaviors of DD32 single crystal superalloy.Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing,592,164-172.
MLA J. J. Yu,et al."High temperature thermo-mechanical and low cycle fatigue behaviors of DD32 single crystal superalloy".Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing 592(2014):164-172.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[J. J. Yu]'s Articles
[G. M. Han]'s Articles
[Z. K. Chu]'s Articles
Baidu academic
Similar articles in Baidu academic
[J. J. Yu]'s Articles
[G. M. Han]'s Articles
[Z. K. Chu]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[J. J. Yu]'s Articles
[G. M. Han]'s Articles
[Z. K. Chu]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.