IMR OpenIR
Low cycle fatigue properties of CLAM steel at 823 K
X. Hu; L. X. Huang; W. Yan; W. Wang; W. Sha; Y. Y. Shan; K. Yang
2014
发表期刊Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing
ISSN0921-5093
卷号613页码:404-413
摘要China Low Activation Martensitic (CLAM) steel is considered to be the main candidate material for the first wall components of future fusion reactors in China. In this paper, the low cycle fatigue (LCF) behavior of CLAM steel is studied under fully reversed tension-compression loading at 823 K in air. Total strain amplitude was controlled from 0.14% to 1.8% with a constant strain rate of 2.4 x 10(-3) s(-1). The corresponding plastic strain amplitude ranged from 0.023% to 1.613%. The CLAM steel displayed continuous softening to failure at 823 K. The relationship between strain, stress and fatigue life was obtained using the parameters obtained from fatigue tests. The LCF properties of CLAM steel at 823 K followed Coffin-Manson relationship. Furthermore, irregular serration was observed on the stress-strain hysteresis loops of CLAM steel tested with the total strain amplitude of 0.45-1.8%, which was attributed to the dynamic strain aging (DSA) effect. During continuous cyclic deformation, the microstructure and precipitate distribution of CLAM steel changed gradually. Many tempered martensitic laths were decomposed into subgrains, and the size and number of M23C6 carbide and MX carbonitride precipitates decreased with the increase of total strain amplitude. The response cyclic stress promoted the recovery of martensitic lath, while the thermal activation mainly played an important role on the growth of precipitates in CLAM steel at 823 K. In order to have a better understanding of high-temperature LCF behavior, the potential mechanisms controlling stress-strain response, DSA phenomenon and microstructure changes have also been evaluated. (C) 2014 Elsevier B.V. All rights reserved.
部门归属[hu, xue ; huang, lixin ; yan, wei ; wang, wei ; shan, yiyin ; yang, ke] chinese acad sci, inst met res, shenyang 110016, peoples r china. [hu, xue] univ chinese acad sci, beijing 100049, peoples r china. [huang, lixin] yanshan univ, state key lab metastable mat sci & technol, qinhuangdao 066004, peoples r china. [sha, wei] queens univ belfast, sch planning architecture & civil engn, belfast bt9 5ag, antrim, north ireland. ; shan, yy (reprint author), chinese acad sci, inst met res, 72 wenhua rd, shenyang 110016, peoples r china. ; yyshan@imr.ac.cn ; kyang@imr.ac.cn
关键词Steel Fatigue Aging Precipitation Electron Microscopy Mechanical Characterization Activation Martensitic Steel Mechanical-properties Room-temperature Jlf-1 Steel Behavior Tensile Tests
URL查看原文
语种英语
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/73242
专题中国科学院金属研究所
推荐引用方式
GB/T 7714
X. Hu,L. X. Huang,W. Yan,et al. Low cycle fatigue properties of CLAM steel at 823 K[J]. Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing,2014,613:404-413.
APA X. Hu.,L. X. Huang.,W. Yan.,W. Wang.,W. Sha.,...&K. Yang.(2014).Low cycle fatigue properties of CLAM steel at 823 K.Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing,613,404-413.
MLA X. Hu,et al."Low cycle fatigue properties of CLAM steel at 823 K".Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing 613(2014):404-413.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[X. Hu]的文章
[L. X. Huang]的文章
[W. Yan]的文章
百度学术
百度学术中相似的文章
[X. Hu]的文章
[L. X. Huang]的文章
[W. Yan]的文章
必应学术
必应学术中相似的文章
[X. Hu]的文章
[L. X. Huang]的文章
[W. Yan]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。