Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air | |
Guan, HR; Li, MJ; Sun, XF | |
Corresponding Author | Guan, HR(hrguan@imr.ac.cn) |
2004 | |
Source Publication | HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS
![]() |
ISSN | 0255-5476 |
Volume | 461-464Pages:417-423 |
Abstract | The morphology evolution of oxide scale formed on the (Ni,Pd)AI coating during oxidation in air at 900 similar to 1100degreesC was investigated systematically by scanning electron microscope and XRD. A long-term observation showed that the transformation of theta- to alpha-Al2O3 occurred on the (Ni,Pd)Al coating with increasing oxidation temperature and time. Furthermore, such transformation is more rapid on the (Ni,Pd)Al coating in comparison to a simple NiAl coating. In addition, the various morphologies for the theta-Al2O3 are also presented in this paper. |
Keyword | (Ni,Pd)Al coating high temperature oxidation transformation theta-Al2O3 alpha-Al2O3 |
Indexed By | SCI |
Language | 英语 |
WOS Research Area | Materials Science ; Metallurgy & Metallurgical Engineering |
WOS Subject | Materials Science, Multidisciplinary ; Metallurgy & Metallurgical Engineering |
WOS ID | WOS:000223339700051 |
Publisher | TRANS TECH PUBLICATIONS LTD |
Citation statistics | |
Document Type | 期刊论文 |
Identifier | http://ir.imr.ac.cn/handle/321006/81415 |
Collection | 中国科学院金属研究所 |
Corresponding Author | Guan, HR |
Affiliation | Chinese Acad Sci, Inst Met Res, Shenyang R&D Ctr Adv Mat, Superalloy Res Div, Shenyang 110016, Peoples R China |
Recommended Citation GB/T 7714 | Guan, HR,Li, MJ,Sun, XF. Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air[J]. HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS,2004,461-464:417-423. |
APA | Guan, HR,Li, MJ,&Sun, XF.(2004).Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air.HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS,461-464,417-423. |
MLA | Guan, HR,et al."Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air".HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS 461-464(2004):417-423. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment