IMR OpenIR
Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application
Li, SJ; Niinomi, M; Akahori, T; Kasuga, T; Yang, R; Hao, YL
通讯作者Niinomi, M(niinomi@sp-mac4.tutpse.tut.ac.jp)
2004-08-01
发表期刊BIOMATERIALS
ISSN0142-9612
卷号25期号:17页码:3369-3378
摘要A new surface-coating method by which CaP invert glass is used to improve the bioactivity of titanium alloys has been developed recently. In this method, the powder of CaP invert glass (CaO-P2O5-TiO2-Na2O) is coated on the surface of titanium alloy samples and heated between 1073 and 1123 K. With this treatment, a calcium phosphate layer mainly containing beta-Ca-3(PO4)(2) phase can be coated easily on titanium alloy samples. In the present study, the effect of this coating process on the fatigue properties of Ti-29Nb-13Ta-4.6Zr, a new metastable beta alloy for biomedical applications, has been investigated. The fatigue endurance limit of the coated alloy was found to be about 15% higher than that of uncoated alloy, as a result of the formation of a hard (alpha + beta) layer and a small amount of the omega phase during the coating process. The coating exhibits excellent adhesion to the substrate during the tensile and fatigue tests. Subsequent ageing at 673 K for 259.2 ks greatly improves the fatigue resistance of the coated alloy due to isothermal omega phase precipitation, and does not have obvious detrimental effect on the coating properties. (C) 2003 Elsevier Ltd. All rights reserved.
关键词titanium alloys biomaterials bioactive coating fatigue
DOI10.1016/j.biomaterials.2003.09.108
收录类别SCI
语种英语
WOS研究方向Engineering ; Materials Science
WOS类目Engineering, Biomedical ; Materials Science, Biomaterials
WOS记录号WOS:000220558200004
出版者ELSEVIER SCI LTD
引用统计
被引频次:56[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/81549
专题中国科学院金属研究所
通讯作者Niinomi, M
作者单位1.Toyohashi Univ Technol, Dept Prod Syst Engn, Toyohashi, Aichi 4418580, Japan
2.Nagoya Inst Technol, Dept Mat Sci, Nagoya, Aichi 4668555, Japan
3.Chinese Acad Sci, Met Res Inst, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Li, SJ,Niinomi, M,Akahori, T,et al. Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application[J]. BIOMATERIALS,2004,25(17):3369-3378.
APA Li, SJ,Niinomi, M,Akahori, T,Kasuga, T,Yang, R,&Hao, YL.(2004).Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application.BIOMATERIALS,25(17),3369-3378.
MLA Li, SJ,et al."Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application".BIOMATERIALS 25.17(2004):3369-3378.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Li, SJ]的文章
[Niinomi, M]的文章
[Akahori, T]的文章
百度学术
百度学术中相似的文章
[Li, SJ]的文章
[Niinomi, M]的文章
[Akahori, T]的文章
必应学术
必应学术中相似的文章
[Li, SJ]的文章
[Niinomi, M]的文章
[Akahori, T]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。