On the critical flow velocity for erosion-corrosion of Ni-based alloys in a saline-sand solution 期刊论文
WEAR, 2020, 卷号: 458, 页码: 10
作者:  Yi, J. Z.;  Hu, H. X.;  Wang, Z. B.;  Zheng, Y. G.
收藏  |  浏览/下载:179/0  |  提交时间:2021/02/02
Ni-based alloy  Erosion-corrosion  Electrochemistry  Passivation  Critical flow velocity  
Dynamic recrystallization initiated by direct grain reorientation at high-angle grain boundary in -titanium 期刊论文
JOURNAL OF MATERIALS RESEARCH, 2019, 卷号: 34, 期号: 9, 页码: 1608-1621
作者:  Wang, Hao;  Bao, Qili L.;  Zhou, Gang;  Qiu, J. K.;  Yang, Yi;  Ma, Y. J.;  Bai, Chunguang G.;  Xu, Dongsheng S.;  Rugg, David;  Huang, Aijun J.;  Hu, Qing-Miao;  Lei, J. F.;  Yang, Rui
收藏  |  浏览/下载:193/0  |  提交时间:2021/02/02
plastic deformation  grain boundary  recrystallization  reorientation  atomistic simulation  
The role of surface film on the critical flow velocity for erosion-corrosion of pure titanium 期刊论文
TRIBOLOGY INTERNATIONAL, 2019, 卷号: 133, 页码: 67-72
作者:  Wang, Z. B.;  Zheng, Y. G.;  Yi, J. Z.
收藏  |  浏览/下载:148/0  |  提交时间:2021/02/02
Erosion-corrosion  Critical flow velocity  Surface film  Depassivation-repassivation  
On the critical flow velocity for erosion-corrosion in local eroded regions under liquid-solid jet impingement 期刊论文
WEAR, 2019, 卷号: 422, 页码: 94-99
作者:  Yi, J. Z.;  Hu, H. X.;  Wang, Z. B.;  Zheng, Y. G.
收藏  |  浏览/下载:123/0  |  提交时间:2021/02/02
Tribo-corrosion  Stainless steel  Erosion-corrosion  Passivation  Critical flow velocity  
On the critical flow velocity for erosion-corrosion in local eroded regions under liquid-solid jet impingement 期刊论文
WEAR, 2019, 卷号: 422, 页码: 94-99
作者:  Yi, J. Z.;  Hu, H. X.;  Wang, Z. B.;  Zheng, Y. G.
收藏  |  浏览/下载:121/0  |  提交时间:2021/02/02
Tribo-corrosion  Stainless steel  Erosion-corrosion  Passivation  Critical flow velocity  
Comparison of critical flow velocity for erosion-corrosion of six stainless steels in 3.5 wt% NaCl solution containing 2 wt% silica sand particles 期刊论文
WEAR, 2018, 卷号: 416, 页码: 62-71
作者:  Yi, J. Z.;  Hu, H. X.;  Wang, Z. B.;  Zheng, Y. G.
收藏  |  浏览/下载:101/0  |  提交时间:2021/02/02
Stainless steels  Erosion-corrosion  Electrochemistry  Passivation  Critical flow velocity  
Comparison of critical flow velocity for erosion-corrosion of six stainless steels in 3.5 wt% NaCl solution containing 2 wt% silica sand particles 期刊论文
WEAR, 2018, 卷号: 416, 页码: 62-71
作者:  Yi, J. Z.;  Hu, H. X.;  Wang, Z. B.;  Zheng, Y. G.
收藏  |  浏览/下载:124/0  |  提交时间:2021/02/02
Stainless steels  Erosion-corrosion  Electrochemistry  Passivation  Critical flow velocity  
The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel 期刊论文
PERGAMON-ELSEVIER SCIENCE LTD, 2017, 卷号: 139, 页码: 188-195
作者:  Fan, Y. H.;  Zhang, B.;  Yi, H. L.;  Hao, G. S.;  Sun, Y. Y.;  Wang, J. Q.;  Han, E. -H.;  Ke, W.;  Zhang, B (reprint author), 62 Wencui Rd, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:137/0  |  提交时间:2018/01/10
Reversed Austenite  Hydrogen Embrittlement  3dap  Fib  Tem  
Preparations and Properties of Amorphous Fe-Mo-B Alloy Deposits by Chemical Plating 期刊论文
Journal of the Electrochemical Society, 2013, 卷号: 160, 期号: 9, 页码: D403-D407
作者:  G. Yi;  B. W. Zhang;  L. L. Wang;  Y. F. Ouyang;  H. W. Xie
收藏  |  浏览/下载:150/0  |  提交时间:2013/12/24
Electroless Nickel  Coatings  Glasses  
CM400马氏体时效钢轴向高频疲劳性能与断裂韧性 会议论文
, 中国陕西西安, 2012
作者:  段启强;  张哲峰;  姚戈;  王中光;  王威;  单以银;  杨柯;  郝遥;  喻家庆
收藏  |  浏览/下载:188/0  |  提交时间:2014/01/10
马氏体时效钢  高频疲劳  疲劳极限  断裂韧性  疲劳断口