IMR OpenIR

浏览/检索结果: 共11条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:

The high-cycle fatigue fracture mechanism and fatigue strength prediction of compacted graphite iron

期刊论文

INTERNATIONAL JOURNAL OF FATIGUE, 2022, 卷号: 161, 页码: 9
作者:  Zou, C. L.;  Pang, J. C.;  Qiu, Y.;  Liu, R.;  Li, S. X.;  Jing, G. X.;  Xu, C. G.;  Zhang, Z. F.
收藏  |  浏览/下载:111/0  |  提交时间:2022/07/14
Compacted graphite iron  Microstructure  High-cycle fatigue  Fracture mechanism  Fatigue strength prediction  
Misorientation dependent thermal condition-solute field cooperative effect on competitive grain growth in the converging case during directional solidification of a nickel-base superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 卷号: 96, 页码: 151-159
作者:  Meng, X. B.;  Li, J. G.;  Jing, C. N.;  Liu, J. D.;  Ma, S. Y.;  Liang, J. J.;  Zhang, C. W.;  Wang, M.;  Tang, B. T.;  Lin, T.;  Chen, J. L.;  Zhang, X. L.;  Li, Q.
收藏  |  浏览/下载:105/0  |  提交时间:2022/07/01
Competitive grain growth  Cooperative effect  Thermal condition  Solute field  Critical misorientation  Unusual overgrowth  Abnormal transformation  
Structural transition in unpoled (1-x)PMN-xPT ceramics near the morphotropic boundary 期刊论文
Journal of Alloys and Compounds, Journal of Alloys and Compounds, 2006, 2006, 卷号: 425, 425, 期号: 1-2, 页码: 373-378, 373-378
作者:  J. B. Li;  G. H. Rao;  G. Y. Liu;  J. R. Chen;  L. Lu;  X. N. Jing;  S. L. Li;  J. K. Liang
收藏  |  浏览/下载:94/0  |  提交时间:2012/04/13
Phase Transition  Phase Transition  X-ray Diffraction  X-ray Diffraction  Dielectric Analysis  Dielectric Analysis  Pb(Mg1/3nb2/3)o-3-Pbtio3  Pb(Mg1/3nb2/3)o-3-Pbtio3  Ferroelectric Phase-transitions  Ferroelectric Phase-transitions  Polarization Rotation  Polarization Rotation  Neutron-diffraction  Neutron-diffraction  Single-crystal  Single-crystal  Perovskites  Perovskites  Stability  Stability  Behavior  Behavior  
Erosion-corrosion of Q235 and 5Cr1/2Mo steels in oil with naphthenic acid and/or sulfur compound at high temperature 期刊论文
Materials and Corrosion-Werkstoffe Und Korrosion, 2005, 卷号: 56, 期号: 8, 页码: 533-541
作者:  D. R. Qu;  Y. G. Zheng;  H. M. Jing;  X. Jiang;  W. Ke
收藏  |  浏览/下载:84/0  |  提交时间:2012/04/14
Mass-spectrometry  Slurry Erosion  Carbon-steel  Petroleum  Synergism  Resistance  Velocity  Wear  
Study on high-temperature naphthenic acid corrosion and erosion-corrosion of aluminized carbon steel 期刊论文
Journal of Materials Science, 2004, 卷号: 39, 期号: 3, 页码: 975-985
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  Z. M. Yao;  W. Ke
收藏  |  浏览/下载:85/0  |  提交时间:2012/04/14
Refineries  
Erosion-corrosion of various oil-refining materials in naphthenic acid 期刊论文
Wear, 2004, 卷号: 256, 期号: 1-2, 页码: 133-144
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  Z. M. Yao;  W. Ke
收藏  |  浏览/下载:105/0  |  提交时间:2012/04/14
Erosion-corrosion  Jet-impingement  Simulation Installation  Naphthenic  Acid Corrosion  Finite-element Analysis  Pitting Corrosion  Rotating Cylinder  Mass-transfer  Refineries  Flow  
Resistance of Mo-bearing stainless steels and Mo-bearing stainless-steel coating to naphthenic acid corrosion and erosion-corrosion 期刊论文
Corrosion Science, 2004, 卷号: 46, 期号: 4, 页码: 1013-1032
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  Z. M. Yao;  W. Ke
收藏  |  浏览/下载:77/0  |  提交时间:2012/04/14
Naphthenic Acid Corrosion  Stainless Steel  Erosion  Hvof Coating  Mo  Pitting Corrosion  Inhibition  Molybdenum  
Corrosion and erosion-corrosion behaviors of carbon steel in naphthenic acid media 期刊论文
Materials and Corrosion-Werkstoffe Und Korrosion, 2002, 卷号: 53, 期号: 11, 页码: 833-844
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  Z. M. Yao;  W. Ke
收藏  |  浏览/下载:75/0  |  提交时间:2012/04/14
Coking of HP tubes in ethylene steam cracking plant and its mitigation 期刊论文
British Corrosion Journal, 2001, 卷号: 36, 期号: 2, 页码: 121-126
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  Z. M. Yao;  W. Ke
收藏  |  浏览/下载:82/0  |  提交时间:2012/04/14
Carbon Deposition  Growth  Nickel  Carburization  Iron  Coke  
Mechanical properties of the industrial HK40 reforming tubes produced by an improved centrifugal processing 期刊论文
Zeitschrift Fur Metallkunde, 2001, 卷号: 92, 期号: 2, 页码: 179-183
作者:  X. Q. Wu;  H. M. Jing;  Y. G. Zheng;  W. Ke;  Y. S. Yang;  Z. Q. Hu
收藏  |  浏览/下载:117/0  |  提交时间:2012/04/14
Mechanical Properties  Reforming Tubes  Electromagnetic Field  Structure  Changes  Electromagnetic-field  Eutectic Alloy  Cast  Microstructure  Flow