A hidden precipitation scenario of the theta'-phase in Al-Cu alloys 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 75, 页码: 126-138
作者:  Zhou, L.;  Wu, C. L.;  Xie, P.;  Niu, F. J.;  Ming, W. Q.;  Du, K.;  Chen, J. H.
收藏  |  浏览/下载:181/0  |  提交时间:2021/10/15
AlCu alloy  Age-hardening  Precipitation  Electron microscopy  
Selective Hydrogenation of Cinnamaldehyde to Cinnamal Alcohol over Platinum/Graphene Catalysts 期刊论文
Chemcatchem, 2014, 卷号: 6, 期号: 11, 页码: 3246-3253
作者:  X. W. Ji;  X. Y. Niu;  B. Li;  Q. Han;  F. L. Yuan;  F. Zaera;  Y. J. Zhu;  H. G. Fu
收藏  |  浏览/下载:130/0  |  提交时间:2015/01/14
Graphene  Heterogeneous Catalysis  Hydrogenation  Platinum  Supported  Catalysts  Reduced Graphene Oxide  Total-energy Calculations  Augmented-wave  Method  Alpha,Beta-unsaturated Aldehydes  Chemoselective Hydrogenation  Unsaturated Aldehydes  Phase Hydrogenation  Supported Platinum  Carbon  Nanotubes  Heterogeneous Catalysis  
The scaling behavior of sputtered Ni3Al coatings with and without Pt modification 期刊论文
Corrosion Science, 2012, 卷号: 58, 页码: 115-120
作者:  J. M. Niu;  W. Wang;  S. L. Zhu;  F. H. Wang
收藏  |  浏览/下载:96/0  |  提交时间:2013/02/05
Platinum  Sputtered Films  Sem  Xrd  Oxidation  High-temperature Oxidation  Al2o3 Scales  Platinum  Alloys  Resistance  Aluminide  Superalloys  Nickel  Interdiffusion  Grain  
Electrodeposition of Ni-SiC nanocomposite film 期刊论文
Transactions of Nonferrous Metals Society of China, 2007, 卷号: 17, 期号: 1, 页码: 41167
作者:  Z. X. Niu;  F. H. Cao;  W. Wang;  Z. Zhang;  J. Q. Zhang;  C. N. Cao
收藏  |  浏览/下载:89/0  |  提交时间:2012/04/13
Ni-sic Nanocomposite Film-  Point Of Zero Charge  Potentiometric  Titration  Electroplating  Nickel  Coatings  Codeposition  Particles  Oxides  Silica  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:103/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
The effect of Cr on the oxidation of Ni-10 at% Al in 1 atm O-2 at 900-1000 degrees C 期刊论文
Oxidation of Metals, 2006, 卷号: 65, 期号: 3-4, 页码: 151-165
作者:  X. J. Zhang;  S. Y. Wang;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:116/0  |  提交时间:2012/04/14
Ternary Alloys  Ni-cr-al  Oxidation  Chromium Effect  Aluminum Alloys  
The third-element effect in the oxidation of Ni-xCr-7Al (x=0, 5, 10 15 at.%) alloys in 1 atm O-2 at 900-1000 degrees C 期刊论文
Corrosion Science, 2006, 卷号: 48, 期号: 12, 页码: 4020-4036
作者:  Y. Niu;  X. J. Zhang;  Y. Wu;  F. Gesmundo
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/14
Ternary Alloys  Ni-cr-al  Oxidation  Third-element Effect  Cr-al Alloys  Most-reactive Component  High Oxidant Pressures  Internal  Oxidation  Ternary Alloys  External Oxidation  High-temperature  Protective Scales  Aluminum Alloys  Binary-alloys  
The third-element effect on the oxidation of Ni-xCr-7Al alloys (x=0, 5, 10 at.%) at 1173K 期刊论文
High Temperature Materials and Processes, 2005, 卷号: 24, 期号: 6, 页码: 369-374
作者:  X. J. Zhang;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:122/0  |  提交时间:2012/04/14
Ternary Alloys  Ni-cr-al  Oxidation  Third-element Effect  Most-reactive Component  1200 Degrees c  Internal Oxidation  Oxidant  Pressures  Ternary Alloys  Al Alloys  Diffusion  Aluminum  Nickel  Oxygen  
The oxidation of two ternary Fe-Cu-10 at.% Al alloys in 1 atm of pure O-2 at 800-900 degrees C 期刊论文
Corrosion Science, 2005, 卷号: 47, 期号: 6, 页码: 1493-1505
作者:  J. H. Xiang;  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/14
Ternary Alloys  Iron-copper Base  Oxidation  Aluminum Effect  Cu-cr Alloys  Forming Insoluble Oxides  2-phase Binary-alloys  Low  Oxidant Pressures  Internal Oxidation  External Oxidation  Air  Oxidation  Approximate Analysis  Ag Alloys  700-900-degrees-c  
Oxidation of the three-phase Cu-20Ni-30Cr and Cu-20Ni-40Cr alloys at 700-800 degrees C in 1 atm O-2 期刊论文
Corrosion Science, 2004, 卷号: 46, 期号: 11, 页码: 2837-2851
作者:  X. J. Zhang;  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:87/0  |  提交时间:2012/04/14
Cu-ni-cr  Ternary Alloys  Three-phase  Oxidation  High Temperature  Most-reactive Component  2-phase Binary-alloys  Air Oxidation  600-800-degrees-c  Corrosion  700-900-degrees-c  Pressures