一种生产高洁净度镁或镁合金的多炉联合式熔铸设备和工艺 专利
专利类型: 发明专利, 专利号: 201610196892.6, 申请日期: 2019-05-07,
发明人:  陈荣石、马跃群、侯丹辉、吴军伟、韩恩厚、柯伟
收藏  |  浏览/下载:99/0  |  提交时间:2021/03/01
Colossal X-Ray-Induced Persistent Photoconductivity in Current-Perpendicular-to-Plane Ferroelectric/Semiconductor Junctions 期刊论文
ADVANCED FUNCTIONAL MATERIALS, 2018, 卷号: 28, 期号: 6, 页码: -
作者:  Hu, WJ;  Paudel, TR;  Lopatin, S;  Wang, ZH;  Ma, H;  Wu, KW;  Bera, A;  Yuan, GL;  Gruverman, A;  Tsymbal, EY;  Wu, T;  Wu, T (reprint author), King Abdullah Univ Sci & Technol, Mat Sci & Engn, Thuwal 239556900, Saudi Arabia.;  Tsymbal, EY (reprint author), Univ Nebraska, Dept Phys & Astron, Lincoln, NE 68588 USA.;  Tsymbal, EY (reprint author), Univ Nebraska, Nebraska Ctr Mat & Nanosci, Lincoln, NE 68588 USA.
收藏  |  浏览/下载:185/0  |  提交时间:2018/06/05
Ferroelectric Tunnel-junctions  Charge-ordered Manganites  Augmented-wave Method  Bifeo3 Thin-films  Oxygen Vacancy  Relaxation  Electroresistance  Semiconductors  Zn0.3cd0.7se  Percolation  
一种净化镁或镁合金熔体的装置 专利
专利类型: 实用新型, 申请日期: 2015-08-05, 公开日期: 2015-08-05
发明人:  陈荣石、马跃群、侯丹辉、吴军伟、柯伟
收藏  |  浏览/下载:99/0  |  提交时间:2017/07/31
硫对Ni-Cr-W-Al高温合金热塑性的影响 期刊论文
热加工工艺, 2013, 期号: 6, 页码: 10-12
作者:  周峰;  高明;  涂赣峰;  刘奎;  彭可武
收藏  |  浏览/下载:124/0  |  提交时间:2013/12/25
金属材料  热塑性  硫含量  Ni-cr-w-al合金  
离心喷射沉积Ti—48Al—2Mn—2Nb的疲劳裂纹扩展速率和门槛值 期刊论文
金属学报, 1998, 卷号: 34.0, 期号: 1.0, 页码: 70-74
作者:  陈文哲;  张飒;  钱匡武;  顾海澄;  王中光
收藏  |  浏览/下载:103/0  |  提交时间:2021/02/02
离心喷射沉积  裂纹扩展速率  门槛值  钛铝合金