IMR OpenIR

浏览/检索结果: 共8条,第1-8条 帮助

已选(0)清除 条数/页:   排序方式:
Effects of exposure temperature and time on corrosion behavior of a ferritic-martensitic steel P92 in aerated supercritical water 期刊论文
Corrosion Science, 2015, 卷号: 90, 页码: 511-521
作者:  X. Y.;  Wu Zhong, X. Q.;  Han, E. H.
收藏  |  浏览/下载:117/0  |  提交时间:2015/05/08
Steel  Sem  High Temperature Corrosion  Oxidation  Bi Eutectic Alloy  Dissolved-oxygen Concentration  Oxide-growth  Mechanisms  316l Stainless-steel  Iron-chromium Alloys  Oxidation  Behavior  Steam Oxidation  Fe-9cr-1mo Steel  In-situ  Elevated-temperatures  
Corrosion behavior of Alloy 690 in aerated supercritical water 期刊论文
Corrosion Science, 2013, 卷号: 66, 页码: 369-379
作者:  X. Y. Zhong;  E. H. Han;  X. Q. Wu
收藏  |  浏览/下载:126/0  |  提交时间:2013/12/24
Alloy  Sem  Xps  High Temperature Corrosion  Oxidation  High-temperature Water  Ni-base Alloys  Oxide-film Formation  X-ray  Photoelectron  Stainless-steel  Iron  Mechanism  Oxidation  Chromium  Diagrams  
Corrosion failure analysis of pure nickel thermocouple sheath used in BaTiO3 hydrothermal synthesis reactor 期刊论文
ENGINEERING FAILURE ANALYSIS, 2010, 卷号: 17, 期号: 6, 页码: 1404-1412
作者:  Zhong, X. Y.;  Wu, X. Q.;  Han, E. H.;  Song, X. B.
收藏  |  浏览/下载:74/0  |  提交时间:2021/02/02
Corrosion failure analysis  Crevice corrosion  Pure Ni  High temperature  High pressure  
Corrosion failure analysis of pure nickel thermocouple sheath used in BaTiO3 hydrothermal synthesis reactor 期刊论文
ENGINEERING FAILURE ANALYSIS, 2010, 卷号: 17, 期号: 6, 页码: 1404-1412
作者:  Zhong, X. Y.;  Wu, X. Q.;  Han, E. H.;  Song, X. B.
收藏  |  浏览/下载:62/0  |  提交时间:2021/02/02
Corrosion failure analysis  Crevice corrosion  Pure Ni  High temperature  High pressure  
Corrosion failure analysis of pure nickel thermocouple sheath used in BaTiO(3) hydrothermal synthesis reactor 期刊论文
Engineering Failure Analysis, 2010, 卷号: 17, 期号: 6, 页码: 1404-1412
作者:  X. Y. Zhong;  X. Q. Wu;  E. H. Han;  X. B. Song
Adobe PDF(1434Kb)  |  收藏  |  浏览/下载:90/0  |  提交时间:2012/04/13
Corrosion Failure Analysis  Crevice Corrosion  Pure Ni  High  Temperature  High Pressure  Crevice Corrosion  Chloride  
Magnetostriction and anisotropy compensation composition of Dy0.9-xTbxPr0.1Fe1.85, Dy1-xTbx(Fe0.9Mn0.1)(1.8) and Dy0.9-xTbxPr0.1(Fe0.9Mn0.1)(1.8) alloys 期刊论文
Journal of Magnetism and Magnetic Materials, 1996, 卷号: 163, 期号: 3, 页码: 360-364
作者:  C. H. Wu;  X. M. Jin;  W. Q. Ge;  Y. C. Chuang;  X. P. Zhong;  R. Q. Li;  J. Y. Li
收藏  |  浏览/下载:113/0  |  提交时间:2012/04/14
Cubic Laves Phase Pseudobinary Compound  Magnetostriction  Anisotropy  Compensation Composition  Iron-aluminum Compounds  Rare-earth  Instability  Tbmn2  
STRUCTURE AND MAGNETOSTRICTION OF DY0.9-XPRXTB0.1FE2 PSEUDOBINARY COMPOUNDS 期刊论文
Journal of Alloys and Compounds, 1993, 卷号: 191, 期号: 2, 页码: 169-171
作者:  C. H. Wu;  W. Q. Ge;  X. M. Jin;  Y. C. Chuang;  X. P. Zhong
收藏  |  浏览/下载:61/0  |  提交时间:2012/04/14
HIGH-FIELD MAGNETIZATION OF PR2(FE,M)14B QUASI-TERNARY COMPOUNDS WITH M = AL, GA AND SI 期刊论文
Journal of the Less-Common Metals, 1991, 卷号: 171, 期号: 2, 页码: 213-219
作者:  X. P. Zhong;  Q. Wang;  C. H. Wu;  F. M. Yang;  N. Tang;  K. H. J. Buschow;  F. R. Deboer
收藏  |  浏览/下载:128/0  |  提交时间:2012/04/14
Crystal  Anisotropy  Pr2fe14b