Study on the oxidation behavior of a novel thermal barrier coating system using the nanocrystalline coating as bonding coating on the single-crystal superalloy 期刊论文
CORROSION SCIENCE, 2023, 卷号: 225, 页码: 12
作者:  Meng, Bo;  Wang, Jinlong;  Chen, Minghui;  Zhu, Shenglong;  Wang, Fuhui
收藏  |  浏览/下载:17/0  |  提交时间:2024/01/07
A. metal coatings  C. oxidation  C. interfaces  A. superalloy