The effect of grain refinement on the oxidation and phase transformation of alumina scale on Ni(2)Al(3 )coating 期刊论文
INTERMETALLICS, 2022, 卷号: 146, 页码: 10
作者:  Khan, A.;  Ullah, Ihsan;  Ullah, A.;  Shah, S. S. A.;  Zhang, S. H.;  Song, G. S.
收藏  |  浏览/下载:140/0  |  提交时间:2022/07/14
Ni 2 Al 3 coating  Grain refinement  SEM  TEM  Raman spectroscopy  Oxidation  Alumina scale formation  
Evaluation of Oxidation of Ti-Al and Ti-Al-Cr Coatings Arc-ion Plated on Ti-60 High-temperature Titanium Alloy 期刊论文
Journal of Materials Science & Technology, 2009, 卷号: 25, 期号: 5, 页码: 637-644
作者:  W. Yan;  Q. J. Wang;  J. R. Liu;  S. Q. Li;  F. J. Sun
Adobe PDF(1261Kb)  |  收藏  |  浏览/下载:69/0  |  提交时间:2012/04/13
Oxidation  Ti-48al Coating  Ti-48al-12cr Coating  High Temperature  Titanium Alloy  Alumina Scale Formation  Resistant Coatings  Behavior  Protection  
Synergistic corrosion behavior of coated Ti60 alloys with NaCl deposit in moist air at elevated temperature 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 1, 页码: 15-22
作者:  Y. M. Xiong;  S. L. Zhu;  F. H. Wang
Adobe PDF(1229Kb)  |  收藏  |  浏览/下载:71/0  |  提交时间:2012/04/13
Titanium  Metal Coatings  X-ray Diffraction  High Temperature Corrosion  Oxide Coatings  Alumina Scale Formation  Oxide hydrOxide Evaporation  Al-cr Alloys  Oxidation Behavior  Water-vapor  Titanium Aluminides  Cyclic Oxidation  Coatings  Chromium  Intermetallics  
Oxidation resistance of ion-implanted gamma-TiAl-base intermetallics 期刊论文
Oxidation of Metals, 2002, 卷号: 58, 期号: 3-4, 页码: 361-374
作者:  M. K. Lei;  X. P. Zhu;  X. J. Wang
收藏  |  浏览/下载:78/0  |  提交时间:2012/04/14
Gamma-tial Intermetallic  Oxidation  Ion implantatIon  Alloying  Thermal Cycle Conditions  Alumina Scale Formation  Al-cr Alloys  Behavior  Niobium  Air  Compound  900-degrees-c  
OXIDATION BEHAVIOR OF TIAL COATED WITH A FINE-GRAIN CO-30CR-4AL FILM 期刊论文
OXIDATION OF METALS, 1993, 卷号: 39, 期号: 5-6, 页码: 457-473
作者:  TANIGUCHI, S;  SHIBATA, T;  ASANUMA, N;  LOU, HY;  WANG, FH;  WU, WT
收藏  |  浏览/下载:139/0  |  提交时间:2021/02/02
HIGH TEMPERATURE  OXIDATION BEHAVIOR  TIAL  CO-CR-AL COATING  ALUMINA SCALE  PORE FORMATION