IMR OpenIR

浏览/检索结果: 共15条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Significantly enhanced resistance to SRB corrosion via Fe-based amorphous coating designed with high dose corrosion-resistant and antibacterial elements 期刊论文
CORROSION SCIENCE, 2020, 卷号: 164, 页码: 9
作者:  Zhang, L. M.;  Yan, M. C.;  Zhang, S. D.;  Zhu, L. Y.;  Umoh, A. J.;  Ma, A. L.;  Zheng, Y. G.;  Wang, J. Q.
收藏  |  浏览/下载:171/0  |  提交时间:2021/02/02
Metal coatings  EIS  TEM  Amorphous structures  Microbiological corrosion  
Thermally induced structure evolution on the corrosion behavior of Al-Ni-Y amorphous alloys 期刊论文
CORROSION SCIENCE, 2018, 卷号: 144, 页码: 172-183
作者:  Zhang, L. M.;  Zhang, S. D.;  Ma, A. L.;  Hu, H. X.;  Zheng, Y. G.;  Yang, B. J.;  Wang, J. Q.
收藏  |  浏览/下载:115/0  |  提交时间:2021/02/02
Aluminum  Polarization  XPS  Amorphous structures  Passive films  
Differences in pitting growth kinetics between Zr60Ni25Al15 and Zr60Cu25Al15 metallic glasses exposed to a 0.6 M NaCl aqueous solution 期刊论文
PERGAMON-ELSEVIER SCIENCE LTD, 2017, 卷号: 128, 页码: 73-84
作者:  Li, Yu;  Xu, Jian;  Xu, J (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, 72 Wenhua Rd, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:145/0  |  提交时间:2018/01/10
Alloy  Zirconium  Polarisation  Amorphous Structures  Kinetic Parameters  Pitting Corrosion  
Effects of the addition of Co, Ni or Cr on the decolorization properties of Fe-Si-B amorphous alloys 期刊论文
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2017, 卷号: 110, 页码: 152-160
作者:  Zhang, Changqin;  Zhu, Zhengwang;  Zhang, Haifeng
收藏  |  浏览/下载:258/0  |  提交时间:2021/02/02
Fe-based amorphous alloys  Surface structures  Decolorization properties  Azo dyes  
Anomalous oxidation of Fe-Si alloys under a low oxygen pressure at 800 degrees C 期刊论文
CORROSION SCIENCE, 2015, 卷号: 98, 页码: 507-515
作者:  Liu, L. L.;  Guo, Q. Q.;  Liu, S.;  Ni, C. S.;  Niu, Y.;  yniu@imr.ac.cn
收藏  |  浏览/下载:113/0  |  提交时间:2016/04/21
Iron  Sem  Internal Oxidation  Amorphous Structures  
Corrosion and erosion-corrosion behaviour of activated combustion high-velocity air fuel sprayed Fe-based amorphous coatings in chloride-containing solutions 期刊论文
CORROSION SCIENCE, 2015, 卷号: 98, 页码: 339-353
作者:  Wang, Y.;  Xing, Z. Z.;  Luo, Q.;  Rahman, A.;  Jiao, J.;  Qu, S. J.;  Zheng, Y. G.;  Shen, J.;  junshen@tongji.edu.cn
收藏  |  浏览/下载:149/0  |  提交时间:2016/04/21
Metal Coatings  Stainless Steel  Erosion  Polarisation  Amorphous Structures  Passivity  
Selective dissolution sensitive to minor alloying in CuZr-based metallic glasses 期刊论文
Corrosion Science, 2013, 卷号: 76, 页码: 465-473
作者:  Z. M. Wang;  X. C. Chang;  W. L. Hou;  J. Q. Wang
收藏  |  浏览/下载:116/0  |  提交时间:2013/12/24
Alloy  Glass  Xps  Amorphous Structures  De-alloying  Corrosion Behavior  Thermal-stability  Hydrochloric-acid  Zr Alloys  Resistance  Elements  Passivity  Nb  Ni  Microscopy  
非晶态结构对锆镍金属玻璃点蚀行为影响的研究 学位论文
, 北京: 中国科学院金属研究所, 2012
作者:  王冬朋
收藏  |  浏览/下载:128/0  |  提交时间:2013/04/12
金属玻璃  非晶态结构  单晶  点蚀  钝化膜  Glass  Amorphous Structures  Single Crystal  Pitting Corrosion  Passive Films  
Exploring Meso-/Microporous Composite Molecular Sieves with Core-Shell Structures 期刊论文
Chemistry-a European Journal, 2012, 卷号: 18, 期号: 3, 页码: 931-939
作者:  X. F. F. Qian;  B. Li;  Y. Y. Y. Hu;  G. X. X. Niu;  Dyhh Zhang;  R. C. C. Che;  Y. Tang;  D. S. S. Su;  A. M. Asiri;  D. Y. Y. Zhao
收藏  |  浏览/下载:115/0  |  提交时间:2013/02/05
Composite Materials  Core-shell Structures  Mesoporous Materials  Molecular Sieves  Zeolites  Amorphous Silica-alumina  Catalytic Cracking  Coke Formation  Zeolite  Mcm-41  Nanoparticles  Fabrication  Oil  Microspheres  Overgrowth  
Corrosion of high-velocity oxy-fuel (HVOF) sprayed iron-based amorphous metallic coatings for marine pump in sodium chloride solutions 期刊论文
Materials and Corrosion-Werkstoffe Und Korrosion, 2012, 卷号: 63, 期号: 8, 页码: 685-694
作者:  Y. Wang;  Y. G. Zheng;  W. Ke;  W. H. Sun;  J. Q. Wang
收藏  |  浏览/下载:103/0  |  提交时间:2013/02/05
Amorphous Structures  Eis  Metallic Coatings  Passivity  Polarization  Stainless Steel  Erosion-corrosion  Stainless-steel  Behavior  Alloys  Resistance  Fe-8cr-13p-7c  Performance  Glasses