Corrosion of Fe-Ni-Cr alloys with various aluminum additions in a carburizing-oxidizing atmosphere at 900 degrees C 期刊论文
CORROSION SCIENCE, 2018, 卷号: 135, 页码: 67-77
作者:  Liu, S;  Shen, J;  Guo, XH;  Liu, LL;  Niu, Y;  Niu, Y (reprint author), Univ Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:107/0  |  提交时间:2018/06/05
Internal Oxidation  External Oxidation  Transition  Mechanism  Resistant  Behavior  Kinetics  Steels  Nickel  Scales  
High-temperature scaling of Cu-Al and Cu-Cr-Al alloys: An example of a non-classical third-element effect 期刊论文
Oxidation of Metals, 2006, 卷号: 65, 期号: 5-6, 页码: 285-306
作者:  Y. Niu;  S. Y. Wang;  F. Gesmundo
收藏  |  浏览/下载:75/0  |  提交时间:2012/04/14
Cu-cr-al  Ternary Alloys  Oxidation  Cr Effect  High Oxidant Pressures  2-phase Binary-alloys  External Oxidation  Solid-solutions  Atm O-2  Copper  Diffusion  Oxides  Scales  Modes  
The third-element effect in the oxidation of Ni-xCr-7Al (x=0, 5, 10 15 at.%) alloys in 1 atm O-2 at 900-1000 degrees C 期刊论文
Corrosion Science, 2006, 卷号: 48, 期号: 12, 页码: 4020-4036
作者:  Y. Niu;  X. J. Zhang;  Y. Wu;  F. Gesmundo
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/14
Ternary Alloys  Ni-cr-al  Oxidation  Third-element Effect  Cr-al Alloys  Most-reactive Component  High Oxidant Pressures  Internal  Oxidation  Ternary Alloys  External Oxidation  High-temperature  Protective Scales  Aluminum Alloys  Binary-alloys  
The internal oxidation of ternary alloys. IV: The internal oxidation of the most-reactive component beneath external scales of the component having intermediate reactivity 期刊论文
Oxidation of Metals, 2004, 卷号: 62, 期号: 5-6, 页码: 357-374
作者:  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:74/0  |  提交时间:2012/04/14
Ternary Alloys  International Oxidation  Most-reactive Component  Kinetics  External Scales  Oxidant Pressures  Legierungen  Oxydation  Bei  
Use of the phase stability and kinetic diagrams in relation to the high temperature oxidation of binary solid-solution alloys 期刊论文
Intermetallics, 2003, 卷号: 11, 期号: 11-12, 页码: 1361-1367
作者:  Y. Niu;  F. Gesmundo;  G. Cacciamani
收藏  |  浏览/下载:80/0  |  提交时间:2012/04/14
Oxidation  Thermodynamic And Thermochemical Properties  High Oxidant Pressures  Forming Insoluble Oxides  Possible Scaling  Modes  Most-stable Oxide  Internal Oxidation  Approximate Analysis  External Oxidation  Scales  Corrosion  Metals