Relationship among fatigue life, inclusion size and hydrogen concentration for high-strength steel in the VHCF regime 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2010, 卷号: 527, 期号: 3, 页码: 559-564
作者:  Z. G. Yang;  S. X. Li;  Y. D. Li;  Y. B. Liu;  W. J. Hui;  Y. Q. Weng
Adobe PDF(882Kb)  |  收藏  |  浏览/下载:80/0  |  提交时间:2012/04/13
High-strength Steel  Granular Bright Facet (Gbf)  Very High Cycle  Fatigue (Vhcf)  Nonmetallic Inclusion  Hydrogen Concentration  High-cycle Fatigue  Subsurface Crack Initiation  Behavior  Surface  Gbf  
Correlations between very high cycle fatigue properties and inclusions of GCr15 bearing steel 期刊论文
ACTA METALLURGICA SINICA, 2008, 卷号: 44, 期号: 8, 页码: 968-972
作者:  Li Yongde;  Yang Zhenguo;  Li Shouxin;  Liu Yangbo;  Chen Shuming
收藏  |  浏览/下载:116/0  |  提交时间:2021/02/02
GCr15 hearing steel  very high cycle fatigue  electroslag remelting  granular-bright facet(GBF)  critical inclusion size  
Estimation of the size of GBF area on fracture surface for high strength steels in very high cycle fatigue regime 期刊论文
International Journal of Fatigue, 2008, 卷号: 30, 期号: 6, 页码: 1016-1023
作者:  Z. G. Yang;  S. X. Li;  Y. B. Liu;  Y. D. Li;  G. Y. Li;  W. J. Hui;  Y. Q. Weng
Adobe PDF(830Kb)  |  收藏  |  浏览/下载:113/0  |  提交时间:2012/04/13
High Strength Steel  Very High Cycle Fatigue  Granular Bright Facet  (Gbf)  Hydrogen  The Maximum Size Of The Plastic Zone  Fatigue Crack  Growth Rate  Subsurface Crack Initiation  Chromium-bearing Steel  Long-life Fatigue  N-greater-than-10(7) Cycles  Part Ii  Mechanism  Failure  Hydrogen  Inclusions  Behavior