Developing novel low-density high-entropy superalloys with high strength and superior creep resistance guided by automated machine learning 期刊论文
ACTA MATERIALIA, 2025, 卷号: 285, 页码: 17
作者:  Li, Yancheng;  Pang, Jingyu;  Li, Zhen;  Wang, Qing;  Wang, Zhenhua;  Li, Jinlin;  Zhang, Hongwei;  Jiao, Zengbao;  Dong, Chuang;  Liaw, Peter K.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
High-entropy superalloys  gamma/gamma' microstructural stability  Mechanical mechanisms  Deformation mechanisms  Machine learning