Effect of high preheating on the microstructure and mechanical properties of high gamma prime Ni-based superalloy manufactured by laser powder bed fusion 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 卷号: 960, 页码: 21
作者:  Chen, Yixuan;  Wang, Weihao;  Ou, Yao;  Li, Daiyun;  Chang, Hai;  Wu, Yingna;  Yang, Rui;  Zhai, Zirong;  Li, Changpeng
收藏  |  浏览/下载:6/0  |  提交时间:2024/01/07
Laser powder bed fusion (L-PBF)  IN738LC superalloy  High preheating  Texture  Anisotropic tensile properties  
Temperature dependence of tensile behavior of Ni-based superalloy M951 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 2008, 卷号: 489, 489, 期号: 1-2, 页码: 227-233, 227-233
作者:  Z. W. Lian;  J. J. Yu;  X. F. Sun;  H. R. Guan;  Z. Q. Hu
Adobe PDF(1739Kb)  |  收藏  |  浏览/下载:99/0  |  提交时间:2012/04/13
M951 Alloy  M951 Alloy  Tensile Strength  Tensile Strength  Ductility  Ductility  Dislocation  Dislocation  Single-crystal Superalloy  Single-crystal Superalloy  Interfacial Dislocation Networks  Interfacial Dislocation Networks  High-volume  High-volume  Fraction  Fraction  Mechanical-properties  Mechanical-properties  Deformation  Deformation  Creep  Creep  Microstructure  Microstructure  In738lc  In738lc  Gamma'  Gamma'  Ni3al  Ni3al  
Thermomechanical fatigue behavior and life prediction of a cast nickel-based superalloy 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2006, 卷号: 432, 期号: 1-2, 页码: 308-316
作者:  Z. W. Huang;  Z. G. Wang;  S. J. Zhu;  F. H. Yuan;  F. G. Wang
收藏  |  浏览/下载:84/0  |  提交时间:2012/04/13
Thermomechanical Fatigue  Isothermal Fatigue  Superalloy  Damage  Mechanism  Life Prediction  Low-cycle-fatigue  High-temperature  Elevated-temperature  Damage  Mechanisms  In738lc  Oxidation  Equations  Mar-m247  Phase