Effect of Zn Additions on the Oxidation of Cu-2 at.% Al and Cu-4 at.% Al Alloys in 1 atm O(2) at 800 A degrees C 期刊论文
Oxidation of Metals, 2009, 卷号: 71, 期号: 1-2, 页码: 43-61
作者:  F. Gao;  F. Gesmundo;  Y. Niu
Adobe PDF(613Kb)  |  收藏  |  浏览/下载:85/0  |  提交时间:2012/04/13
Third-element Effect  Oxidation  Cu-zn-al Alloys  Most-reactive Component  Intermediate Oxidant Pressures  Alpha-solid-solutions  External Oxidation  Ternary Alloys  Internal  Oxidation  Transition  Copper  Diffusion  Kinetics  
The effect of Si additions on the high-temperature oxidation of a ternary Ni-10Cr-4Al alloy in 1 ATM O(2) AT 900-1000 degrees C 期刊论文
Oxidation of Metals, 2008, 卷号: 69, 期号: 5-6, 页码: 299-315
作者:  S. Wang;  Y. Wu;  F. Gesmundo;  Y. Niu
Adobe PDF(942Kb)  |  收藏  |  浏览/下载:96/0  |  提交时间:2012/04/13
Ni-cr-si-al Alloys  Oxidation  Third-element Effect  Intermediate Oxidant Pressures  Most-reactive Components  1200 Degrees  c  Internal Oxidation  External Oxidation  Transition  At.percent  Silicon  X=0  
The internal oxidation of ternary alloys. VI: The transition from internal to external oxidation of the most-reactive component under intermediate oxidant pressures 期刊论文
Oxidation of Metals, 2004, 卷号: 62, 期号: 5-6, 页码: 391-410
作者:  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:70/0  |  提交时间:2012/04/14
Internal Oxidation  Ternary Alloys  High Temperatures  Intermediate  Oxidant Pressures  
The internal oxidation of ternary alloys II: The coupled internal oxidation of the two most-reactive components under intermediate oxidant pressures 期刊论文
Oxidation of Metals, 2003, 卷号: 60, 期号: 5-6, 页码: 371-391
作者:  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:85/0  |  提交时间:2012/04/14
Ternary Alloys  Double Internal Oxidation  Intermediate Oxidant  Pressures  Nickel-base Alloys  External Scale  Si Alloys  Ni  Al  Diffusion  Kinetics  Nitridation  Behavior  System