IMR OpenIR

浏览/检索结果: 共12条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Cyclic hot corrosion behavior and mechanism of GH4738 superalloy in mixed molten salt 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 卷号: 32, 页码: 3456-3464
作者:  Xin, Dan;  Huang, Hailiang;  Yang, Yanhong;  Wang, Guanglei;  Qu, Jinglong;  Chen, Yang;  Wu, Chongchong;  Zhao, Jiankang;  Wang, Yinuo;  Ma, Wenting
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
GH4738 superalloy  Molten salt  Cyclic hot corrosion  
Cyclic hot corrosion behavior and mechanism of GH4738 superalloy in mixed molten salt 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 卷号: 32, 页码: 3456-3464
作者:  Xin, Dan;  Huang, Hailiang;  Yang, Yanhong;  Wang, Guanglei;  Qu, Jinglong;  Chen, Yang;  Wu, Chongchong;  Zhao, Jiankang;  Wang, Yinuo;  Ma, Wenting
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
GH4738 superalloy  Molten salt  Cyclic hot corrosion  
Effect of tantalum and Ni-Ta barriers on inter-diffusion between nickel coating and GH3535 alloy at 700 & DEG;C 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2023, 卷号: 467, 页码: 10
作者:  Wang, Chengxu;  Zhu, Jiahui;  Song, Yaqi;  Liu, Zhongli;  Chen, Wei;  Chen, Demin
收藏  |  浏览/下载:12/0  |  提交时间:2024/01/08
Diffusion  Barrier  Superalloy  Molten salt reactor  
Ni/AlN Composite Coating for Corrosion and Elements Interdiffusion Resistance in Molten Fluoride Salts System 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 页码: 11
作者:  Wang, Chengxu;  Chen, Wei;  Chen, Minghui;  Chen, Demin;  Wang, Fuhui
收藏  |  浏览/下载:117/0  |  提交时间:2021/10/15
Molten salt  Superalloy  Composite coating  High temperature corrosion  
Preparation of alumina/aluminide coatings on molybdenum metal substrates, and protection performance evaluation utilizing a DZ40M superalloy casting test 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2020, 卷号: 395, 页码: 15
作者:  Zheng, Liwei;  Liu, Enze;  Zheng, Zhi;  Ning, Likui;  Tong, Jian;  Tan, Zheng
收藏  |  浏览/下载:129/0  |  提交时间:2021/02/02
Refractory metal core  Superalloy  Pack cementation  Investment casting  High temperature oxidation  Molten metal corrosion  
Preparation of alumina/aluminide coatings on molybdenum metal substrates, and protection performance evaluation utilizing a DZ40M superalloy casting test 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2020, 卷号: 395, 页码: 15
作者:  Zheng, Liwei;  Liu, Enze;  Zheng, Zhi;  Ning, Likui;  Tong, Jian;  Tan, Zheng
收藏  |  浏览/下载:141/0  |  提交时间:2021/02/02
Refractory metal core  Superalloy  Pack cementation  Investment casting  High temperature oxidation  Molten metal corrosion  
Effects of yttrium on wettability and interactions between molten superalloy and SiO2-based ceramic core 期刊论文
CERAMICS INTERNATIONAL, 2020, 卷号: 46, 期号: 6, 页码: 7324-7335
作者:  Zi, Yun;  Meng, Jie;  Zou, Mingke;  Xu, Wei;  Li, Jinguo;  Xu, Ke;  Zhou, Yizhou;  Ding, Yutian
收藏  |  浏览/下载:122/0  |  提交时间:2021/02/02
Molten superalloy  SiO2-based ceramic core  High-temperature wettability  Interface reaction  Yttrium  
High-temperature corrosion behavior of sputtered K38 nanocrystalline coatings with and without yttrium addition in molten sulfate at 900 degrees C 期刊论文
Surface & Coatings Technology, 2011, 卷号: 206, 期号: 1, 页码: 68-74
作者:  P. Yu;  W. Wang;  F. H. Wang;  S. L. Zhu
Adobe PDF(3186Kb)  |  收藏  |  浏览/下载:122/0  |  提交时间:2012/04/13
K38 Superalloy  Nanocrystalline Coating  Yttrium  Molten Sulfate  High  Temperature Corrosion  Oxidation Behavior  Hot-corrosion  Resistance  Alloys  Scales  K38g  
Preparation and hot corrosion behaviour of a MCrAlY plus AlSiY composite coating 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 11, 页码: 3213-3220
作者:  S. M. Jiang;  X. Peng;  Z. B. Bao;  S. C. Liu;  Q. M. Wang;  J. Gong;  C. Sun
Adobe PDF(1431Kb)  |  收藏  |  浏览/下载:101/0  |  提交时间:2012/04/13
Superalloy  Metal Coatings  Molten Salts  Hot Corrosion  Gradient Nicocralysib Coatings  Oxidation Behavior  Nacl  In-738lc  Silicon  
Long-term hot corrosion behavior of Ni-based superalloy M38G using electrochemical impedance spectroscopy 期刊论文
High Temperature Materials and Processes, 2006, 卷号: 25, 期号: 4, 页码: 187-195
作者:  C. L. Zeng;  J. Li
收藏  |  浏览/下载:98/0  |  提交时间:2012/04/14
Ni-based Superalloy M38g  (Na  k)(2)So4  Hot Corrosion  Electrochemical  Impedance  Molten-salt Corrosion  Na2so4 Film  Degrees-c  Electrode  Air