The strength-ductility balance of Al0.4CoCu0.6NiTix (x <= 1.0) and Al0.4CoCu0.6NiSi0.2Tix (x <= 0.5) high entropy alloys by regulating the proportion of Ti and improving the cooling rate 期刊论文
VACUUM, 2018, 卷号: 155, 页码: 270-279
作者:  Chen, Yongxing;  Zhu, Sheng;  Wang, Xiaoming;  Yang, Baijun;  Ren, Zhiqiang;  Han, Guofeng;  Wen, Shu
收藏  |  浏览/下载:114/0  |  提交时间:2021/02/02
High entropy alloys  Elements addition  Rapid cooling  Phase transformation  Strength-ductility balance  
The strength-ductility balance of Al0.4CoCu0.6NiTix (x <= 1.0) and Al0.4CoCu0.6NiSi0.2Tix (x <= 0.5) high entropy alloys by regulating the proportion of Ti and improving the cooling rate 期刊论文
VACUUM, 2018, 卷号: 155, 页码: 270-279
作者:  Chen, Yongxing;  Zhu, Sheng;  Wang, Xiaoming;  Yang, Baijun;  Ren, Zhiqiang;  Han, Guofeng;  Wen, Shu
收藏  |  浏览/下载:101/0  |  提交时间:2021/02/02
High entropy alloys  Elements addition  Rapid cooling  Phase transformation  Strength-ductility balance  
A bridge from monotectic alloys to liquid-phase-separated bulk metallic glasses: Design, microstructure and phase evolution 期刊论文
Acta Materialia, 2013, 卷号: 61, 期号: 6, 页码: 2102-2112
作者:  J. He;  N. Mattem;  J. Tan;  J. Z. Zhao;  I. Kaban;  Z. Wang;  L. Ratke;  D. H. Kim;  W. T. Kim;  J. Eckert
收藏  |  浏览/下载:124/0  |  提交时间:2013/12/24
Monotectic Solidification  Bulk Metallic Glasses  Phase Separation  Rapid Solidification  Microstructure  In-situ Formation  Al-co Alloy  Nb-y Alloy  Cooling Rate  Ni Alloys  Fe  Alloys  Solidification  Behavior  Stability  Temperature