IMR OpenIR

浏览/检索结果: 共3条,第1-3条 帮助

已选(0)清除 条数/页:   排序方式:
Surface recrystallisation and oxidation of polycrystalline superalloy castings during isothermal exposure at 1100 degrees C 期刊论文
International Journal of Cast Metals Research, 2012, 卷号: 25, 期号: 4, 页码: 195-200
作者:  W. G. Jiang;  M. C. Yang;  L. H. Lou;  Z. Q. Hu
收藏  |  浏览/下载:99/0  |  提交时间:2013/02/05
Superalloy  Investment Casting  Modulus  Recrystallisation  Residual  Stress  Oxidation  Ni-base Superalloy  Gas-turbine Blade  Heat-treatment  Dynamic  Recrystallization  Leading-edge  Water-vapor  Microstructure  Behavior  900-degrees-c  Evolution  
Improved solution treatment for an as-rolled Al-Zn-Mg-Cu alloy. Part II. Microstructure and mechanical properties 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 534, 页码: 244-252
作者:  D. K. Xu;  P. A. Rometsch;  N. Birbilis
收藏  |  浏览/下载:138/0  |  提交时间:2013/02/05
Solution Treatment  Constituent Particle  Dissolution Kinetics  Recrystallisation  Aa7150  Aluminum-alloys  Fracture-toughness  Heat-treatment  Process Model  Si-cu  Precipitation  Behavior  Strength  Dissolution  Cracking  
Mechanical behaviour of Zr doped Ni3Al alloy: effects of heat treatment, environment, and temperature 期刊论文
Materials Science and Technology, 2005, 卷号: 21, 期号: 7, 页码: 824-830
作者:  Y. F. Li;  J. T. Guo;  H. Q. Ye
收藏  |  浏览/下载:58/0  |  提交时间:2012/04/14
Ni3al(Zr) Alloy  Mechanical Properties  Environmental Embrittlement  Recrystallisation Treatment  Low-expansion Superalloy  Embrittlement  Dependence  Ductility