IMR OpenIR

浏览/检索结果: 共16条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Effect of brazing temperature and brazing time on the microstructure and tensile strength of TiAl-based alloy joints with Ti-Zr-Cu-Ni amorphous alloy as filler metal 期刊论文
ELSEVIER SCI LTD, 2017, 卷号: 91, 页码: 35-44
作者:  Cai, Y. S.;  Liu, R. C.;  Zhu, Z. W.;  Cui, Y. Y.;  Yang, R.;  Cui, YY (reprint author), Chinese Acad Sci, Inst Met Res, 72 Wenhua Rd, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:274/0  |  提交时间:2018/01/10
Vacuum Brazing  Titanium Aluminide  Microstructure  Bonding Strength Test  Amorphous Ti-37.5zr-15cu-15ni Brazing Alloy  
Effects of casting temperature on the microstructure and mechanical properties of the TiZr-based bulk metallic glass matrix composite 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2014, 卷号: 589, 页码: 182-188
作者:  P. F. Sha;  Z. W. Zhu;  H. M. Fu;  H. Li;  A. M. Wang;  H. W. Zhang;  H. F. Zhang;  Z. Q. Hu
收藏  |  浏览/下载:164/0  |  提交时间:2014/02/19
Bulk Metallic Glass  Composite  Casting Temperature  Cooling Rate  Oxygen Content  Thermal-stability  Zr41.2ti13.8cu12.5ni10.0be22.5  Crystallization  Oxygen  Plasticity  Kinetics  Liquid  Alloy  Phase  Dendrites  
Structure of Bergman-type W-TiZrNi approximants to quasicrystal, analyzed by lattice inversion method 期刊论文
Journal of Physics-Condensed Matter, 2014, 卷号: 26, 期号: 31
作者:  H. Huang;  D. Q. Meng;  X. C. Lai;  T. W. Liu;  Y. Long;  Q. M. Hu
收藏  |  浏览/下载:166/0  |  提交时间:2015/01/14
W-tizrni Approximant  Lattice Inversion  Site Preference  Phase  Stability  Ti-zr-ni  Molecular-dynamics Simulation  Interatomic Potentials  Atomistic Simulation  Site Preference  Transition  Stability  Hydrogen  Program  Storage  
Preparation, microstructure and deformation behavior of Zr-based metallic glass/porous SiC interpenetrating phase composites 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2011, 卷号: 530, 页码: 15-20
作者:  Y. L. Chen;  A. M. Wang;  H. M. Fu;  Z. W. Zhu;  H. F. Zhang;  Z. Q. Hu;  L. Wang;  H. W. Cheng
收藏  |  浏览/下载:98/0  |  提交时间:2012/04/13
Composite Materials  Metallic Glasses  Porous Preforms  Mechanical  Properties  Fracture Behavior  Glass-matrix-composites  Mechanical-properties  Pressureless  Infiltration  Fracture-behavior  Failure Behavior  Forming Alloy  Tungsten  Ceramics  Zr41ti14cu12ni10be23  Preforms  
Ti_(43.5)Ni_(47.0)Nb_(9.0)Zr_(0.5)合金的相变和记忆功能 期刊论文
中国有色金属学报, 2010, 期号: S1, 页码: 463-467
作者:  王健;  张慧博;  金伟;  刘羽寅
收藏  |  浏览/下载:78/0  |  提交时间:2012/04/12
Ti_(43.5)Ni_(47.0)Nb_(9.0)Zr_(0.5)合金  热拉  相变  记忆功能  
金属熔滴在基片上方和基片下方的润湿性研究 期刊论文
表面技术, 2009, 期号: 2, 页码: 4-6+16
作者:  张波;  李文;  李宏
收藏  |  浏览/下载:97/0  |  提交时间:2012/04/12
润湿  重力  Zr41.2ti13.8cu12.5ni10.0be22.5合金熔体  Sic基片  
Complete Composition Tunability of Cu(Ni)-Ti-Zr Alloys 期刊论文
Journal of Materials Science & Technology, 2009, 卷号: 25, 期号: 1, 页码: 39-47
作者:  Z. X. Zhang;  C. L. Dai;  J. Xu
Adobe PDF(1761Kb)  |  收藏  |  浏览/下载:97/0  |  提交时间:2012/04/13
Bulk Metallic Glasses  Amorphous Alloys  Eutectic  Copper  Glass-forming Ability  Bulk Metallic-glass  Cu-ti-zr  Eutectic Reaction  Amorphous-alloys  System  Ni  Si  Plasticity  Diameter  
Comparison of bulk metallic glass formation between Cu-Hf binary and Cu-Hf-Al ternary alloys 期刊论文
Journal of Materials Research, 2009, 卷号: 24, 期号: 1, 页码: 96-106
作者:  P. Jia;  J. Xu
Adobe PDF(1389Kb)  |  收藏  |  浏览/下载:107/0  |  提交时间:2012/04/13
Supercooled Liquid Region  Mold Casting Method  Ni-nb-sn  Forming  Ability  Zr-ti  Mechanical-properties  Amorphous-alloys  Thermal-stability  Eutectic Reaction  Critical Size  
A group of Cu(Zr)-based BMGs with critical diameter in the range of 12 to 18 mm 期刊论文
Journal of Materials Science & Technology, 2008, 卷号: 24, 期号: 2, 页码: 149-152
作者:  Y. Shen;  E. Ma;  J. Xu
Adobe PDF(4881Kb)  |  收藏  |  浏览/下载:77/0  |  提交时间:2012/04/13
Bulk Metallic Glasses  Glass-forming Ability  Copper  Zirconium  Bulk Metallic Glasses  Forming Ability  Cu-zr  Thermal-stability  Alloys  Ni  Plasticity  Ag  Ti  
Wetting behavior of CuZr-based BMGs/alumina system 期刊论文
Journal of Alloys and Compounds, 2008, 卷号: 462, 期号: 1-2, 页码: 343-346
作者:  G. F. Ma;  H. F. Zhang;  H. Li;  Z. Q. Hu
Adobe PDF(461Kb)  |  收藏  |  浏览/下载:106/0  |  提交时间:2012/04/13
Wetting  Interface  Bulk Metallic Glass  Alumina  Bulk Metallic-glass  Spreading Kinetics  Composites  Tungsten  Zr41.2ti13.8cu12.5ni10.0be22.5  Wettability  Alloys  Al