Development of a nickel-base cast superalloy with high strength and superior creep properties 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 卷号: 21, 期号: 3, 页码: 347-352
作者:  Hou, JS;  Guo, JT;  Zhou, LZ;  Li, ZJ
收藏  |  浏览/下载:115/0  |  提交时间:2021/02/02
conventional Ni-base superalloy  tensile strength  creep life  PHACOMP