Microstructure and mechanical properties evolutions of 9Cr heat resistant steel deposited metals with different Si contents during 550 °C aging process 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 卷号: 26, 页码: 2122-2139
作者:  Yu, Tongtong;  Liu, Chen;  Wu, Dong;  Wei, Shitong;  Lu, Shanping
收藏  |  浏览/下载:10/0  |  提交时间:2024/01/08
Silicon content  Tensile strength  Impact toughness  High temperature aging  Post weld heat treatment  Deposited metal  
Variation of microstructure and composition of the Cr(2)AlC coating prepared by sputtering at 370 and 500 degrees C 期刊论文
Surface & Coatings Technology, 2010, 卷号: 204, 期号: 23, 页码: 3838-3845
作者:  J. J. Li;  L. F. Hu;  F. Z. Li;  M. S. Li;  Y. C. Zhou
Adobe PDF(707Kb)  |  收藏  |  浏览/下载:84/0  |  提交时间:2012/04/13
Cr(2)Alc Coating  Alpha-(Cr  Max Phase  Al)(2)o(3)  Magnetron Sputtering  Microstructure  Substrate Temperature  Phase Thin-films  Ab-initio Calculations  Select Max Phases  Tribological Behavior  m(n+1)Ax(n) Phases  Deposited Chromium  Oxidation  Behavior  Vapor Deposits  Nitride Films  Bulk Cr2alc  
Calculation on deposited temperature during pulsed bias arc ion plating 期刊论文
ACTA METALLURGICA SINICA, 2004, 卷号: 40, 期号: 10, 页码: 1069-1073
作者:  Bai, X;  Lin, GQ;  Dong, C;  Wen, LS
收藏  |  浏览/下载:97/0  |  提交时间:2021/02/02
arc ion plating  pulsed bias  deposited temperature  calculation