Influence of Ru on the thermomechanical fatigue deformation behavior of a single crystal superalloy 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2022, 卷号: 156, 页码: 10
作者:  Ge, Zhicheng;  Xie, Guang;  Segersall, Mikael;  Norman, Viktor;  Chen, Zhe;  Moverare, Johan;  Lou, Langhong;  Zhang, Jian
收藏  |  浏览/下载:116/0  |  提交时间:2022/07/01
Nickel-base superalloy  Single crystal  Thermomechanical fatigue  Ru  Twinning  
High temperature shakedown of a 2nd generation nickel-base single crystal superalloy under tension-torsion loadings 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 卷号: 832, 页码: 12
作者:  Zhang, Zhen;  Wang, Shen;  Brown, Bailey;  Cinoglu, I. Soner;  Vermaak, Natasha;  Lou, Langhong;  Zhang, Jian
收藏  |  浏览/下载:122/0  |  提交时间:2022/07/01
Shakedown  Nickel-base single crystal superalloy  Cyclic loading  Mechanical behavior  
Prediction of Primary Dendrite Arm Spacing in Pulsed Laser Surface Melted Single Crystal Superalloy 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2020, 页码: 10
作者:  Ci, Shiwei;  Liang, Jingjing;  Li, Jinguo;  Wang, Haiwei;  Zhou, Yizhou;  Sun, Xiaofeng;  Zhang, Hongwei;  Ding, Yutian;  Zhou, Xin
收藏  |  浏览/下载:163/0  |  提交时间:2021/02/02
Additive manufacturing  Nickel-base superalloy  Single crystal  Pulsed laser  Primary dendritic arm spacing  
Cyclic inelastic behavior and shakedown response of a 2nd generation nickel-base single crystal superalloy under tension-torsion loadings: Experiments and simulations 期刊论文
EUROPEAN JOURNAL OF MECHANICS A-SOLIDS, 2020, 卷号: 80, 页码: 10
作者:  Zhang, Zhen;  Cinoglu, I. Soner;  Charbal, Ali;  Vermaak, Natasha;  Lou, Langhong;  Zhang, Jian
收藏  |  浏览/下载:171/0  |  提交时间:2021/02/02
Shakedown  Inelastic design  Cyclic loading  Elastic-perfectly-plastic  Nickel-base single crystal superalloy  Tension-torsion loadings  
Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 789, 页码: 472-484
作者:  Zi, Yun;  Meng, Jie;  Zhang, Chaowei;  Yang, Yanhong;  Zhou, Yizhou;  Ding, Yutian
收藏  |  浏览/下载:136/0  |  提交时间:2021/02/02
Nickel-base single crystal superalloy melt  Ceramic mould  Interface reaction  Wettability  Y content  
Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 789, 页码: 472-484
作者:  Zi, Yun;  Meng, Jie;  Zhang, Chaowei;  Yang, Yanhong;  Zhou, Yizhou;  Ding, Yutian
收藏  |  浏览/下载:130/0  |  提交时间:2021/02/02
Nickel-base single crystal superalloy melt  Ceramic mould  Interface reaction  Wettability  Y content  
Dislocation Structure in a Single Crystal Nickel Base Superalloy During High Cycle Fatigue at 870 degrees C 期刊论文
RARE METAL MATERIALS AND ENGINEERING, 2018, 卷号: 47, 期号: 4, 页码: 1054-1058
作者:  Shui Li;  Xu Yunchao;  Hu Zhuangqi
收藏  |  浏览/下载:146/0  |  提交时间:2021/02/02
nickel base single crystal superalloy  high cycle fatigue  dislocation  
Influence of Heat Treatment on gamma ' Phase and Property of a Directionally Solidified Superalloy 期刊论文
HIGH TEMPERATURE MATERIALS AND PROCESSES, 2018, 卷号: 37, 期号: 3, 页码: 271-276
作者:  Xia, PC;  Xie, K;  Cui, HZ;  Yu, JJ;  Xia, PC (reprint author), Shandong Univ Sci & Technol, Sch Mat Sci & Engn, Qingdao 266590, Peoples R China.
收藏  |  浏览/下载:99/0  |  提交时间:2018/06/05
Nickel-base Superalloy  Single-crystal Superalloy  Microstructure  Mechanisms  Alloy  Generations  
Dislocation motion during high-temperature low-stress creep in Ru-free and Ru-containing single-crystal superalloys 期刊论文
Materials & Design, 2015, 卷号: 67, 页码: 543-551
作者:  X. G.;  Liu Wang, J. L.;  Jin, T.;  Sun, X. F.;  Hu, Z. Q.;  Do, J. H.;  Choi, B. G.;  Kim, I. S.;  Jo, C. Y.
收藏  |  浏览/下载:138/0  |  提交时间:2015/05/08
Ni-base Single Crystal Superalloy  Creep Behavior  Dislocation  Structure  Transmission Electron Microscopy  Nickel-base Superalloys  Gamma'-volume Fraction  Internal-stresses  Phase-stability  Lattice Misfit  Evolution  Additions  Behavior  Microstructure  Deformation  
Influence of microstructures on thermal fatigue property of a nickel-base superalloy 期刊论文
Frontiers of Materials Science, 2015, 卷号: 9, 期号: 1, 页码: 85-92
作者:  P. C.;  Chen Xia, F. W.;  Xie, K.;  Qiao, L.;  Yu, J. J.
收藏  |  浏览/下载:142/0  |  提交时间:2015/05/08
Nickel-base Superalloy  Thermal Fatigue  Microstructure  Crack  High-temperature  Single-crystal  Behavior