IMR OpenIR

浏览/检索结果: 共11条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Effects of phosphorus and boron on the γ " precipitate evolution and creep properties of IN718 superalloy during long-term thermal exposure at 680 °C 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 995, 页码: 12
作者:  Wang, Zhiyuan;  Xue, Chaochao;  Liu, Yingjie;  Xin, Xin;  Sun, Wenru
收藏  |  浏览/下载:1/0  |  提交时间:2025/04/27
IN718 superalloy  Phosphorus and boron  Long-term thermal exposure  gamma '' precipitates  Creep property  
Effect of P and B compound strengthening on the evolution of phases and stress rupture properties of the IN718 superalloy during long-term aging at 650 & DEG;C 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 卷号: 881, 页码: 14
作者:  Wang, Zhiyuan;  Zhang, Weiwei;  Li, Shaowei;  Mei, Feiqiang;  Xin, Xin;  Sun, Wenru
收藏  |  浏览/下载:17/0  |  提交时间:2024/01/08
IN718 superalloy  Phosphorus and boron compound  strengthening  Long -term aging  Microstructure  Stress-rupture property  
Re-recognition of the Effects of Phosphorus and Boron on the gamma '' and gamma ' Phases in IN718 Alloy 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  Zhang, An-Wen;  Li, Yang;  Zhang, Sha;  Liu, Fang;  Zhang, Wei-Hong;  Yu, Lian-Xu;  Sun, Wen-Ru
收藏  |  浏览/下载:116/0  |  提交时间:2021/02/02
IN718 superalloy  Phosphorus and boron  gamma '' and gamma ' phases  Hardness  
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings 期刊论文
ACTA METALLURGICA SINICA, 2019, 卷号: 55, 期号: 9, 页码: 1160-1174
作者:  Bi Zhongnan;  Qin Hailong;  Dong Zhiguo;  Wang Xiangping;  Wang Ming;  Liu Yongquan;  Du Jinhui;  Zhang Ji
收藏  |  浏览/下载:175/0  |  提交时间:2021/02/02
TEMPERATURE STRUCTURE STABILITY  SITU NEUTRON-DIFFRACTION  IN-SITU  SINGLE-CRYSTAL  CREEP-BEHAVIOR  TURBINE DISC  INCONEL 718  RELAXATION  MICROSTRUCTURE  DISTORTION  superalloy  residual stress  neutron diffraction  contour method  turbine disk  
Re-recognition of the Effects of Phosphorus and Boron on the γ'' and γ' Phases in IN718 Alloy 期刊论文
Acta Metallurgica Sinica(English Letters), 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  Zhang Anwen;  Li Yang;  Zhang Sha;  Liu Fang;  Zhang Weihong;  Yu Lianxu;  Sun Wenru
收藏  |  浏览/下载:124/0  |  提交时间:2021/02/02
IN718 superalloy  Phosphorus and boron  γ'' and γ' phases  Hardness  
Re-recognition of the Effects of Phosphorus and Boron on the γ'' and γ' Phases in IN718 Alloy 期刊论文
Acta Metallurgica Sinica(English Letters), 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  Zhang Anwen;  Li Yang;  Zhang Sha;  Liu Fang;  Zhang Weihong;  Yu Lianxu;  Sun Wenru
收藏  |  浏览/下载:123/0  |  提交时间:2021/02/02
IN718 superalloy  Phosphorus and boron  γ'' and γ' phases  Hardness  
Grain refinement of as cast superalloy K4169 solidified with low voltage pulsed magnetic field 期刊论文
Materials Research Innovations, 2014, 卷号: 18, 页码: 352-356
作者:  Y. F.;  Feng Teng, X. H.;  Li, Y. J.;  Yang, Y. S.
收藏  |  浏览/下载:132/0  |  提交时间:2015/05/08
Grain Refinement  Superalloy  Pulsed Magnetic Field  Solidification  Magnesium Alloy  In718  Al  
Refinement Mechanism of Low Voltage Pulsed Magnetic Field on Solidification Structure of Silicon Steel 期刊论文
Metals and Materials International, 2014, 卷号: 20, 期号: 3, 页码: 527-530
作者:  Y. J. Li;  Y. F. Teng;  Y. S. Yang
收藏  |  浏览/下载:121/0  |  提交时间:2015/01/14
Alloys  Casting  Grain Refinement  Computer Simulation  Low Voltage  Pulsed Magnetic Field  Grain-refinement  Superalloy In718  Stainless-steel  Microstructure  Alloy  Al  
Hot die forging process optimization of superalloy IN718 turbine disc using processing map and finite element method 期刊论文
Proceedings of the Institution of Mechanical Engineers Part B-Journal of Engineering Manufacture, 2010, 卷号: 224, 期号: B1, 页码: 103-110
作者:  H. Y. Zhang;  S. H. Zhang;  Z. X. Li;  M. Cheng
Adobe PDF(446Kb)  |  收藏  |  浏览/下载:93/0  |  提交时间:2012/04/13
Superalloy In718  Turbine Disc  Processing Map  Finite Element Method  Microstructure Simulation  High-temperature Deformation  Metadynamic Recrystallization  Microstructural Evolution  Flow Behavior  Inconel-718  Working  Simulation  In-718  
Effect of temperature and strain amplitude on dislocation structure of M963 superalloy during high-temperature low cycle fatigue 期刊论文
Materials Transactions, 2006, 卷号: 47, 期号: 1, 页码: 67-71
作者:  L. Z. He;  Q. Zheng;  X. F. Sun;  H. R. Guan;  Z. Q. Hu;  K. Tieu;  C. Lu;  H. T. Zhu
收藏  |  浏览/下载:91/0  |  提交时间:2012/04/13
M963 Superalloy  Low Cycle Fatigue (Lcf)  Temperature  Strain Amplitude  Dislocation Structure  Ni-base Superalloy  Single-crystal Superalloy  Crystallographic  Orientation  Deformation-behavior  In-100 Superalloy  Room-temperature  Stainless-steel  Inconel 718  Creep  Morphology