Comparison of the Three-Phase Corrosion Behavior of SiN and 304L Stainless Steels in 6 M Nitric Acid Solution at Different Temperatures 期刊论文
METALS, 2022, 卷号: 12, 期号: 6, 页码: 17
作者:  Sun, Shengxuan;  Zhang, Lianmin;  Ma, Aili;  Daniel, Enobong Felix;  Zhang, Chunzhi;  Zheng, Yugui
收藏  |  浏览/下载:94/0  |  提交时间:2022/09/16
stainless steel  three-phase corrosion behavior  nitric acid  weight loss  corrosion kinetics  