Effects of Al on microstructural stability and related stress-rupture properties of a third-generation single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 卷号: 35, 期号: 11, 页码: 2537-2542
Authors:  Sun, Jingxia;  Liu, Jinlai;  Liu, Lirong;  Zhou, Yizhou;  Li, Jinguo;  Sun, Xiaofeng
Favorite  |  View/Download:9/0  |  Submit date:2020/01/06
Ni base single crystal superalloys  Thermal exposure  Microstructural stability  Stress-rupture property  Al  
Influences of Re on low-cycle fatigue behaviors of single crystal superalloys at intermediate temperature 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 卷号: 35, 期号: 9, 页码: 1917-1924
Authors:  Liu, Liu;  Meng, Jie;  Liu, Jinlai;  Zou, Mingke;  Zhang, Haifeng;  Sun, Xudong;  Zhou, Yizhou
Favorite  |  View/Download:8/0  |  Submit date:2020/01/06
Single crystal superalloys  Low-cycle fatigue  Deformation behaviors  Deformation mechanisms  
Effects of Ta on the solidification behavior and microstructure of a rhenium-containing hot corrosion resistant single crystal 期刊论文
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 卷号: 26, 期号: 7, 页码: 901-907
Authors:  Ma, Shi-hua;  Hao, Hong-quan;  Wang, Dong;  Lou, Lang-hong;  Zhang, Jian
Favorite  |  View/Download:5/0  |  Submit date:2020/01/06
superalloys  tantalum  solidification behavior  microstructure  
Intergrowth of P phase with Laves phase C36 in the high Mo-containing nickel-base single crystal superalloy 期刊论文
MATERIALS RESEARCH EXPRESS, 2019, 卷号: 6, 期号: 4
Authors:  Ma, Shiyu;  Zhang, Jianxin;  Li, Pan;  Zhang, Youjian;  Jin, Huixin;  Zhang, Wenyang;  Li, Xueqiao;  Mao, Shengcheng;  Liu, Jide;  Wang, Xinguang;  Zhou, Yizhou;  Sun, Xiaofeng;  Ni, Wei
Favorite  |  View/Download:6/0  |  Submit date:2020/01/06
nickel-base single crystal superalloys  Laves phase  P phase  intergrowth  HRTEM  
Growth twins of R phase in the high Mo-containing nickel-base single crystal superalloy 期刊论文
MATERIALS RESEARCH EXPRESS, 2018, 卷号: 5, 期号: 12, 页码: -
Authors:  Ma, SY;  Zhang, JX;  Li, P;  Zhang, YJ;  Jin, HX;  Zhang, WY;  Li, XQ;  Mao, SC;  Liu, JD;  Wang, XG;  Zhou, YZ;  Sun, XF;  Ni, W
Favorite  |  View/Download:6/0  |  Submit date:2018/12/25
nickel-base single crystal superalloys  R phase  growth twins  microstructure  
Atomic arrangement and formation of planar defects in the mu phase of Ni-base single crystal superalloys 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 卷号: 766, 页码: 775-783
Authors:  Ma, SY;  Li, XQ;  Zhang, JX;  Liu, JD;  Li, P;  Zhang, YJ;  Jin, HX;  Zhang, WY;  Zhou, YZ;  Sun, XF;  Zhang, Q;  Chen, YH;  Mao, SC
Favorite  |  View/Download:7/0  |  Submit date:2018/12/25
Ni-base single crystal superalloys  mu phase  Planar defects  HAADF-STEM  Atomic arrangement characteristics  
Atomic-scale observation and analysis of chemical ordering in M3B2 and M5B3 borides 期刊论文
ACTA MATERIALIA, 2018, 卷号: 149, 页码: 274-284
Authors:  Hu, XB;  Niu, HY;  Ma, XL;  Oganov, AR;  Fisher, CAJ;  Sheng, NC;  Liu, JD;  Jin, T;  Sun, XF;  Liu, JF;  Ikuhara, Y;  Ma, XL (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Liaoning, Peoples R China.;  Ikuhara, Y (reprint author), Japan Fine Ceram Ctr, Nanostruct Res Lab, Nagoya, Aichi 4568587, Japan.;  Oganov, AR (reprint author), SUNY Stony Brook, Inst Adv Computat Sci, Ctr Mat By Design, Dept Geosci, Stony Brook, NY 11794 USA.
Favorite  |  View/Download:30/0  |  Submit date:2018/06/05
Crystal-structure Prediction  Total-energy Calculations  Nickel-base Superalloys  Ni-based Superalloy  X-ray Spectroscopy  Wave Basis-set  Probe Tomography  Polycrystalline Superalloy  Grain-boundary  Resolution  
Intergrowth of C phase within mu phase in a Re-containing Ni-base single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 卷号: 34, 期号: 5, 页码: 806-810
Authors:  Gao, S;  Zhou, YZ;  Liu, ZQ;  Jin, T;  Liu, ZQ (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China.
Favorite  |  View/Download:32/0  |  Submit date:2018/06/05
Nickel-based Superalloys  Close-packed Phase  Rhenium Additions  Creep Resistance  Precipitation  Cmsx-4  Co7w6  
A phase-field model for creep behavior in nickel-base single-crystal superalloy: Coupled with creep damage 期刊论文
SCRIPTA MATERIALIA, 2018, 卷号: 147, 页码: 16-20
Authors:  Yang, M;  Zhang, J;  Wei, H;  Gui, WM;  Su, HJ;  Jin, T;  Liu, L;  Zhang, J (reprint author), Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Shaanxi, Peoples R China.;  Jin, T (reprint author), Chinese Acad Sci, Inst Met Res, Superalloys Div, Shenyang 110016, Liaoning, Peoples R China.
Favorite  |  View/Download:32/0  |  Submit date:2018/06/05
Ni-based Superalloys  Deformation  Simulation  Transformations  Plasticity  Evolution  Alloys  
Effects of Re on surface eutectic formation for Ni-base single crystal superalloys during directional solidification 期刊论文
JOURNAL MATER SCI TECHNOL, 2017, 卷号: 33, 期号: 11, 页码: 1308-1313
Authors:  Cao, Liang;  Zhou, Yizhou;  Jin, Tao;  Sun, Xiaofeng;  Zhou, YZ (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China.
Favorite  |  View/Download:49/0  |  Submit date:2018/01/10
Surface Eutectic  Re Addition  Single Crystal  Superalloy