| Effects of grain refinement on the microstructure and tensile behavior of K417G superalloy 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2015, 卷号: 623, 页码: 59-67 Authors: B. N.; Yang Du, J. X.; Cui, C. Y.; Sun, X. F.
 Favorite  |  View/Download:106/0  |  Submit date:2015/05/08 Nickel Superalloy Grain Refinement Microstructure Tensile Properties Intermediate-temperature Embrittlement Nickel-base Superalloy High-cycle Fatigue Stress-rupture Heat-treatment Alloy Ni Mechanisms Size Resistance |
| Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2014, 卷号: 599, 页码: 186-195 Authors: L. T. Chang; W. R. Sun; Y. Y. Cui; R. Yang
 Favorite  |  View/Download:91/0  |  Submit date:2014/07/03 Powder Metallurgy Superalloy Hot-isostatic-pressing Prior Particle Boundary Carbide Tensile Fracture Nickel-base Superalloy Mechanical-properties Heat-treatment Alloy Solidification Phosphorus Particles Parts Hip |
| Effect of revert addition on microstructure and mechanical properties of M951 Ni-base superalloy 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 532, 页码: 41437 Authors: Y. H. Yang; J. J. Yu; X. F. Sun; T. Jin; H. R. Guan; Z. Q. Hu
 Favorite  |  View/Download:114/0  |  Submit date:2013/02/05 Ni-base Superalloy Recycled Superalloy Mechanical Property Foam Ceramic Filter Nickel-based Superalloy Nitrogen Boron Temperature Inclusions Behavior |
| Fatigue crack growth behavior of a newly developed Ni-Co-base superalloy TMW-2 at elevated temperatures 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 552, 页码: 464-471 Authors: Z. H. Zhong; Y. F. Gu; Y. Yuan; C. Y. Cui; T. Yokokawa; H. Harada
 Favorite  |  View/Download:73/0  |  Submit date:2013/02/05 Fatigue Crack Growth Ni-base Superalloys Temperature Effect Load Ratio Effect Nickel-based Superalloy Wave-form Creep Micromechanisms Frequency Oxidation Alloy Ratio |
| Effect of NiCrAlY platelets inclusion on the mechanical and thermal shock properties of glass matrix composites 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2011, 卷号: 528, 期号: 3, 页码: 1360-1366 Authors: M. H. Chen; S. L. Zhu; M. L. Shen; F. H. Wang; Y. Niu
Adobe PDF(1284Kb)  |   Favorite  |  View/Download:110/0  |  Submit date:2012/04/13 Mechanical Characterization Micromechanics Glass Nickel Based Superalloys Sintering Fracture Hot Corrosion Behavior Nickel-base Superalloy Fracture-toughness Metallic Particles Oxidation Coatings Al Microstructure Intermetallics Adherence |
| Effects of different C contents on the microstructure, tensile properties and stress-rupture properties of IN792 alloy 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2011, 卷号: 528, 期号: 3, 页码: 1534-1539 Authors: J. X. Yang; Q. Zheng; M. Q. Ji; X. F. Sun; Z. Q. Hu
Adobe PDF(2577Kb)  |   Favorite  |  View/Download:67/0  |  Submit date:2012/04/13 Superalloy Carbides Grain Boundary Stress-rupture Properties Nickel-base Superalloy Mc Carbide Solidification Fatigue |
| The effects of Co and Ti additions on microstructures and compressive strength of Udimet710 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2011, 卷号: 528, 期号: 27, 页码: 7851-7856 Authors: L. Xu; C. Y. Cui; X. F. Sun
Adobe PDF(1455Kb)  |   Favorite  |  View/Download:71/0  |  Submit date:2012/04/13 Ni-base Superalloy Eta Phase (Eta) Gamma ' Morphology Yield Strength Nickel-base Superalloys Phase |
| Properties and microstructures of M951 alloy after long-term exposure 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2010, 卷号: 527, 期号: 7-8, 页码: 1896-1902 Authors: J. J. Yu; Z. W. Lian; Z. K. Chu; X. F. Sun; H. R. Guan; Z. Q. Hu
Adobe PDF(2086Kb)  |   Favorite  |  View/Download:61/0  |  Submit date:2012/04/13 M951 Superalloy Heat Treatment Long-term Ageing Yield Strength Stress Rupture Life Ni-base Superalloy Nickel-based Superalloy Temperature-dependence Mechanical-properties Thermal Exposure Precipitation Growth Boron |
| Effects of heat treatments on the microstructure of IN792 alloy 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2010, 卷号: 527, 期号: 4-5, 页码: 1016-1021 Authors: J. X. Yang; Q. Zheng; H. Y. Zhang; X. F. Sun; H. R. Guan; Z. Q. Hu
Adobe PDF(1749Kb)  |   Favorite  |  View/Download:64/0  |  Submit date:2012/04/13 Superalloy Heat Treatment Carbides Gamma ' Phase Nickel-based Superalloys Ni-base Superalloy K465 Superalloy Phase Carbide |
| Effect of surface recrystallization on the creep rupture properties of a nickel-base single crystal superalloy 期刊论文 Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2010, 卷号: 527, 期号: 23, 页码: 6119-6122 Authors: J. Meng; T. Jin; X. F. Sun; Z. Q. Hu
Adobe PDF(527Kb)  |   Favorite  |  View/Download:53/0  |  Submit date:2012/04/13 Nickel-base Single Crystal Superalloy Recrystallization Creep Microstructural Evolution Mechanical-properties Boundaries Behavior Cmsx-2 |